			<title type="html"><![CDATA[Re: massive oozing]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/41100/#p41100" />
			<content type="html"><![CDATA[<p>Sounds like filament contaminant.... moisture?</p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2013-11-09T00:42:05Z</updated>
			<id>https://www.soliforum.com/post/41100/#p41100</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: massive oozing]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/41096/#p41096" />
			<content type="html"><![CDATA[<p>Yea, extruder turns off. I&#039;m only concerned because it never used to do that. It kind of seems like the longer a print goes now, the oozier it gets. For example, 30 minutes into a print there are more blobs and strings than earlier. Again, never really happened like that before. Was usually much more consistent through the whole print.</p>]]></content>
			<author>
				<name><![CDATA[muddtt]]></name>
				<uri>https://www.soliforum.com/user/3491/</uri>
			</author>
			<updated>2013-11-09T00:01:54Z</updated>
			<id>https://www.soliforum.com/post/41096/#p41096</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: massive oozing]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/41094/#p41094" />
			<content type="html"><![CDATA[<p>Do you have it set to turn off the extruder heat off/down after the print completes? If so then maybe add a some post print gcode to retract and relieve the back pressure. For the most part I never complain about free flowing filament, considering the alternative.</p>]]></content>
			<author>
				<name><![CDATA[foofoodog]]></name>
				<uri>https://www.soliforum.com/user/3054/</uri>
			</author>
			<updated>2013-11-08T23:47:00Z</updated>
			<id>https://www.soliforum.com/post/41094/#p41094</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[massive oozing]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/40997/#p40997" />
			<content type="html"><![CDATA[<p>Dunno what&#039;s happening, but lately it seems like the SD has been oozing a lot more than usual. For example, in the picture below this is how much oozes out after a print completes. It&#039;s never been that long before. At most in the past it&#039;s just been a little curl that might come out 1/4 of an inch. I&#039;m even down to printing at 180 degrees for ABS. Maybe the consistency of this Sainsmart roll is changing? or anyone else have any thoughts?</p><p><span class="postimg"><img src="http://img833.imageshack.us/img833/8435/ov1o.jpg" alt="http://img833.imageshack.us/img833/8435/ov1o.jpg" /></span></p>]]></content>
			<author>
				<name><![CDATA[muddtt]]></name>
				<uri>https://www.soliforum.com/user/3491/</uri>
			</author>
			<updated>2013-11-08T04:40:41Z</updated>
			<id>https://www.soliforum.com/post/40997/#p40997</id>
		</entry>
</feed>