<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Slic3r Port Disconnect (Stopping mid-print)]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/4385/" />
	<updated>2013-10-28T19:29:25Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/4385/slic3r-port-disconnect-stopping-midprint/</id>
		<entry>
			<title type="html"><![CDATA[Slic3r Port Disconnect (Stopping mid-print)]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/40159/#p40159" />
			<content type="html"><![CDATA[<p>I&#039;ve been having trouble with my brand new solidoodle 2. Almost every print that I&#039;ve printed lately has been ruined by the fact that my printer suddenly stops and loses connection with my computer. I click disconnect and reconnect and then I get the message, &quot;the port does not exist.&quot; I have tried everything from plugging the printer straight into the wall to changing the baud rate to 25,000. I am using a computer that I built last summer and using windows 7. It&#039;s really frustrating me and discouraging me from printing anything remotely large because I&#039;m tired of wasting plastic and time. I know that I may have a faulty usb cable or faulty drivers at this time, but I don&#039;t know how to fix the drivers.&nbsp; The RH log screen says nothing when the printer disconnects. The printer just stops mid-print and when I try to control the printer manually it doesn&#039;t respond. The only way that I can get the printer to connect again is by clicking disconnect in RH and then unplug/replug in the usb cable to my computer and then hit connect in RH again. If I do not unplug/replug the usb cable and just hit disconnect/connect I get the message &quot;The port does not exist.&quot; Its very frustrating stuff. It doesn&#039;t look as if any damage has been done to the motherboard and the packaging looked well done with no damage done to the box when I received it. Any help is greatly appreciated.</p>]]></content>
			<author>
				<name><![CDATA[PandolarBear]]></name>
				<uri>https://www.soliforum.com/user/3611/</uri>
			</author>
			<updated>2013-10-28T19:29:25Z</updated>
			<id>https://www.soliforum.com/post/40159/#p40159</id>
		</entry>
</feed>