		<entry>
			<title type="html"><![CDATA[Re: Black stuff coming out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/36840/#p36840" />
			<content type="html"><![CDATA[<p>I&#039;ll take some more pictures tonight. But I know it&#039;s not the extruder bumping because I&#039;ve seen the black actually come out when I&#039;m just manually extruding with no print. It seems to be a little rarer As of last night though. Also there kind of a burning smell...</p>]]></content>
			<author>
				<name><![CDATA[Madhatter]]></name>
				<uri>https://www.soliforum.com/user/2001/</uri>
			</author>
			<updated>2013-09-19T22:02:51Z</updated>
			<id>https://www.soliforum.com/post/36840/#p36840</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Black stuff coming out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/36788/#p36788" />
			<content type="html"><![CDATA[<p>can we get more pictures on the print?? i am trying to see if it&#039;s the print head bumping into bumps and burning the print. when you print does the bed vibrates a lot? like a bumpy road? if thats the case, you might need to calibrate your extrusion.</p><p>and the black mark on your nozzle.. it&#039;s normal. if sand paper is too big to sand that small area, you can use knife to scrap it off. watch for the wires.</p>]]></content>
			<author>
				<name><![CDATA[RavensCrest]]></name>
				<uri>https://www.soliforum.com/user/651/</uri>
			</author>
			<updated>2013-09-19T13:04:58Z</updated>
			<id>https://www.soliforum.com/post/36788/#p36788</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Black stuff coming out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/36785/#p36785" />
			<content type="html"><![CDATA[<p>I tried two filaments a while back. Trying another tonight. Still sends to be occasionally letting out some black. Almost like oil...</p>]]></content>
			<author>
				<name><![CDATA[Madhatter]]></name>
				<uri>https://www.soliforum.com/user/2001/</uri>
			</author>
			<updated>2013-09-19T10:34:59Z</updated>
			<id>https://www.soliforum.com/post/36785/#p36785</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Black stuff coming out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/36784/#p36784" />
			<content type="html"><![CDATA[<p>My nozzle looks like that. But I do not have black stuff in my prints. It is probably contaminants inside the current filament you are using. Change filament and purge it to find out.</p>]]></content>
			<author>
				<name><![CDATA[Hazer]]></name>
				<uri>https://www.soliforum.com/user/2747/</uri>
			</author>
			<updated>2013-09-19T09:29:43Z</updated>
			<id>https://www.soliforum.com/post/36784/#p36784</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Black stuff coming out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/36775/#p36775" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>saymo606 wrote:</cite><blockquote><p>looks normal to me...use a fine grade sandpaper on the nozzle, comes off no problem..</p></blockquote></div><p>Hmm...I&#039;ll try this tonight, I think the black crap is actually inside though as well...</p>]]></content>
			<author>
				<name><![CDATA[Madhatter]]></name>
				<uri>https://www.soliforum.com/user/2001/</uri>
			</author>
			<updated>2013-09-19T03:57:30Z</updated>
			<id>https://www.soliforum.com/post/36775/#p36775</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Black stuff coming out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/36774/#p36774" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>ronsii wrote:</cite><blockquote><p>Have you ever used a different color filament in that extruder? any evidence of impurities in the filament roll you are using... and what kind of filament?</p></blockquote></div><p>Yeah, I have several colours.<br />I bought white abs once, that was very brittle, and didn&#039;t print well. Maybe that has left black crap in the nozzle?</p><p>I use both ABS and PLA.</p>]]></content>
			<author>
				<name><![CDATA[Madhatter]]></name>
				<uri>https://www.soliforum.com/user/2001/</uri>
			</author>
			<updated>2013-09-19T03:56:48Z</updated>
			<id>https://www.soliforum.com/post/36774/#p36774</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Black stuff coming out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/35668/#p35668" />
			<content type="html"><![CDATA[<p>looks normal to me...use a fine grade sandpaper on the nozzle, comes off no problem..</p>]]></content>
			<author>
				<name><![CDATA[saymo606]]></name>
				<uri>https://www.soliforum.com/user/456/</uri>
			</author>
			<updated>2013-09-09T11:49:35Z</updated>
			<id>https://www.soliforum.com/post/35668/#p35668</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Black stuff coming out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/35590/#p35590" />
			<content type="html"><![CDATA[<p>Have you ever used a different color filament in that extruder? any evidence of impurities in the filament roll you are using... and what kind of filament?</p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2013-09-09T01:10:45Z</updated>
			<id>https://www.soliforum.com/post/35590/#p35590</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Black stuff coming out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/35539/#p35539" />
			<content type="html"><![CDATA[<p>looks like soot to me.</p>]]></content>
			<author>
				<name><![CDATA[MolecularConcept]]></name>
				<uri>https://www.soliforum.com/user/2211/</uri>
			</author>
			<updated>2013-09-08T17:34:15Z</updated>
			<id>https://www.soliforum.com/post/35539/#p35539</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Black stuff coming out]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/35498/#p35498" />
			<content type="html"><![CDATA[<p>Hey,</p><p>So my soli 2 has been leaking black gunk into the prints. It&#039;s not burning the tops of the plastic or anything, I&#039;ve actually seen little specs of black coming out of the nozzle while printing.<br />I&#039;m assuming other people here have had the same problem at some point?</p><p>Anyone that can point me in the right direction for cleaning tips, or how to fix this would be greatly appreciated, thank you so much!</p>]]></content>
			<author>
				<name><![CDATA[Madhatter]]></name>
				<uri>https://www.soliforum.com/user/2001/</uri>
			</author>
			<updated>2013-09-08T06:42:00Z</updated>
			<id>https://www.soliforum.com/post/35498/#p35498</id>
		</entry>