<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Loose print head, broken extruder parts]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/3778/" />
	<updated>2013-09-02T22:17:17Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/3778/loose-print-head-broken-extruder-parts/</id>
		<entry>
			<title type="html"><![CDATA[Loose print head, broken extruder parts]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/35015/#p35015" />
			<content type="html"><![CDATA[<p>On the last few prints I noticed that I was getting some banding, not horrible, but still somewhat noticeable.&nbsp; And considering I had already replaced the original Z Screw with a ball screw, I had no idea where I was getting that from.</p><p>So last night while I was printing a few small things, I noticed that the print head was actually moving slightly on its platform.&nbsp; The 2 vertical screws that hold the horizontal &quot;tail piece&quot; to the main/front sliding block were loose and the entire head assembly was wobbly because of it.&nbsp; But when I removed the screws to get to the 2 loose ones, I realized that the wood piece that holds the hot end in place was also very loose, so I had to disassemble the print head.</p><p>When I took off the screws that hold the extruder to the motor, 3 or 4 pieces of the plexiglass layers came off.&nbsp; These were the right corner pieces that have hold the wood platform screw in place and they had broken off.&nbsp; Only one plexi layer was still intact.&nbsp; I glued the pieces back, and also glued the back 3 layers together and the front 3 layers together, so they&#039;re stronger now, but I think I&#039;ll be printing a different print head to replace this one.</p><p>Anyway, after I got everything together, I printed a test print, and as far as I can tell, the banding is gone.</p><p>All things considered, I think that Solidoodle should reconsider the design of the print head from a more structural angle.&nbsp; Yeah, it looks cool being transparent, but it has a lot of weak areas that are under stress, so they&#039;re likely to break sooner or later.&nbsp; Or at least they should glue some of these layers together to give them strength.&nbsp; The way it was designed, you don&#039;t need all the parts separate, the back 3 layers can be glued together, and the front three can be glued together, then everything can be assembled together with the captive screws in place.</p>]]></content>
			<author>
				<name><![CDATA[pirvan]]></name>
				<uri>https://www.soliforum.com/user/1357/</uri>
			</author>
			<updated>2013-09-02T22:17:17Z</updated>
			<id>https://www.soliforum.com/post/35015/#p35015</id>
		</entry>
</feed>