<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — crumbly support material on .1mm resolution prints]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/3611/" />
	<updated>2013-08-20T00:35:20Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/3611/crumbly-support-material-on-1mm-resolution-prints/</id>
		<entry>
			<title type="html"><![CDATA[Re: crumbly support material on .1mm resolution prints]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/33604/#p33604" />
			<content type="html"><![CDATA[<p>For infill, I&#039;ve noticed that problem too. </p><p>Perhaps you can change the slic3r setting &quot;infill every X layers&quot; to &quot;3&quot; because that is a good way to speed up .1mm prints, and might result in something more similar to the .3mm infill.</p>]]></content>
			<author>
				<name><![CDATA[Tomek]]></name>
				<uri>https://www.soliforum.com/user/192/</uri>
			</author>
			<updated>2013-08-20T00:35:20Z</updated>
			<id>https://www.soliforum.com/post/33604/#p33604</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[crumbly support material on .1mm resolution prints]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/33594/#p33594" />
			<content type="html"><![CDATA[<p>hello everybody, so i went through got everything sorted out and was getting more beautiful prints in .3 and .2mm resolution than i&#039;d ever gotten before. so now i&#039;m tackling .1mm last because it takes the longest and isn&#039;t as important to me as the other two settings i listed. so i everything runs great on the prints and actually the prints turn out fine, but the infill and support material don&#039;t really turn out that great, the actual print runs fine though. the inside of my prints looks more like a sponge than a set of hexagons and the support material just sort of bunches up all over and really doesn&#039;t help anything. i&#039;m not really sure why its not working so great, my one idea is that the print head is moving to fast, but the last thing i want to do is further slow down the .1mm setting lol... any ideas? i already set the width to the magic 1.4x the layer height (which helps a lot).</p>]]></content>
			<author>
				<name><![CDATA[michael.rosplock]]></name>
				<uri>https://www.soliforum.com/user/2962/</uri>
			</author>
			<updated>2013-08-19T23:19:37Z</updated>
			<id>https://www.soliforum.com/post/33594/#p33594</id>