			<title type="html"><![CDATA[Re: Essential kit]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/30284/#p30284" />
			<content type="html"><![CDATA[<p>This is the case I&#039;ve started building. All the tools will go into a bag that sits under my printer. This case just keeps all the smaller/more fragile parts in their own little containers. I still haven&#039;t filled it completely, but it&#039;s getting there.</p>]]></content>
			<author>
				<name><![CDATA[pretenda]]></name>
				<uri>https://www.soliforum.com/user/231/</uri>
			</author>
			<updated>2013-07-19T11:57:27Z</updated>
			<id>https://www.soliforum.com/post/30284/#p30284</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Essential kit]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/30045/#p30045" />
			<content type="html"><![CDATA[<p>I use acid brushes or&nbsp; 45 cal. cleaning patches with hemostats in the acetone</p>]]></content>
			<author>
				<name><![CDATA[dubbsd]]></name>
				<uri>https://www.soliforum.com/user/187/</uri>
			</author>
			<updated>2013-07-16T23:00:50Z</updated>
			<id>https://www.soliforum.com/post/30045/#p30045</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Essential kit]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/30041/#p30041" />
			<content type="html"><![CDATA[<p>I&#039;ve got a small brush I use to paint it on parts (rather than having them sit in a vapor bath).&nbsp; But I&#039;ve also used an old tee-shirt with a bit of acetone on it to clean the bed and nozzle.</p>]]></content>
			<author>
				<name><![CDATA[mconsidine]]></name>
				<uri>https://www.soliforum.com/user/1122/</uri>
			</author>
			<updated>2013-07-16T22:17:53Z</updated>
			<id>https://www.soliforum.com/post/30041/#p30041</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Essential kit]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/30040/#p30040" />
			<content type="html"><![CDATA[<p>Awesome, thanks guys. Loads of great ideas. I can&#039;t believe I forgot to write acetone. I have a 1L bottle in front of me. What do you normally apply acetone with? A small brush?</p>]]></content>
			<author>
				<name><![CDATA[pretenda]]></name>
				<uri>https://www.soliforum.com/user/231/</uri>
			</author>
			<updated>2013-07-16T21:48:36Z</updated>
			<id>https://www.soliforum.com/post/30040/#p30040</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Essential kit]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/30032/#p30032" />
			<content type="html"><![CDATA[<p>i use razor scrapper, to clean bed and remove item.. kidna like the paint scrapper, but with sharp edge.<br />and I have a tweezer uts long enough to reach hotend without touching belt and heatbed. (kinda like the one in solidoodle&#039;s video)</p>]]></content>
			<author>
				<name><![CDATA[RavensCrest]]></name>
				<uri>https://www.soliforum.com/user/651/</uri>
			</author>
			<updated>2013-07-16T20:10:29Z</updated>
			<id>https://www.soliforum.com/post/30032/#p30032</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Essential kit]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/30011/#p30011" />
			<content type="html"><![CDATA[<p>Acetone for cleaning nozzle if printing ABS<br />White lithium grease<br />Multimeter</p>]]></content>
			<author>
				<name><![CDATA[mconsidine]]></name>
				<uri>https://www.soliforum.com/user/1122/</uri>
			</author>
			<updated>2013-07-16T16:04:02Z</updated>
			<id>https://www.soliforum.com/post/30011/#p30011</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Essential kit]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/30008/#p30008" />
			<content type="html"><![CDATA[<p>spare connectors (JST, MTA-100 or other) <br />spare Epcos NTC 100K Thermistor<br />some high temp 20-24 awg wire</p><p>If you are looking for minimal downtime then it&#039;s nice to have either a spare power supply or a power supply that is over kill so you don&#039;t have to worry about one dying.</p>]]></content>
			<author>
				<name><![CDATA[2n2r5]]></name>
				<uri>https://www.soliforum.com/user/1906/</uri>
			</author>
			<updated>2013-07-16T15:12:57Z</updated>
			<id>https://www.soliforum.com/post/30008/#p30008</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Essential kit]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/30002/#p30002" />
			<content type="html"><![CDATA[<p>Spare Pololu A4988 or equivalent (DRV8825 etc). Nothing worse than when a dead driver.<br />Extra heater cartridge (assuming the first time your resistor burns out, you swap to a more reliable cartridge)</p>]]></content>
			<author>
				<name><![CDATA[adrian]]></name>
				<uri>https://www.soliforum.com/user/663/</uri>
			</author>
			<updated>2013-07-16T14:17:20Z</updated>
			<id>https://www.soliforum.com/post/30002/#p30002</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Essential kit]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/30001/#p30001" />
			<content type="html"><![CDATA[<p>I like to have one complete hot end ready to go. That way if I get a clog, I just swap out the hot end and continue without having to sped a bunch of time trying to unclog. </p><p>A paint scraper and tweezers are in my kit.</p>]]></content>
			<author>
				<name><![CDATA[downeym]]></name>
				<uri>https://www.soliforum.com/user/1737/</uri>
			</author>
			<updated>2013-07-16T14:15:35Z</updated>
			<id>https://www.soliforum.com/post/30001/#p30001</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Essential kit]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/30000/#p30000" />
			<content type="html"><![CDATA[<p>Hey everyone,</p><p>Im in the process of sorting out my tool cases and was looking at building one solely for my printer. What are some of the things you can&#039;t do without? At the moment I&#039;m thinking the following;</p><p>Spares:<br />A complete set of printed parts (x, y carriages, extruder etc)<br />Appropriate bearings for these carriages<br />Spare 40mm fans<br />Assortment of m3 screws and nuts<br />Bulldog clips for beds<br />Glass beds<br />Garolite bed<br />Extruder parts (I plan on installing the e3d, so the complete original solidoodle extruder)<br />Nozzles<br />5x5 flex coupler (just cause I ordered spares)</p><p>Tools:<br />Hex drivers<br />Flat blade screwdrivers<br />Various knives<br />Digital vernier calipers<br />Side cutters<br />Small pliers<br />Small shifter</p><p>Consumables:<br />Kapton tape (I have 6mm)<br />Blue painters tape<br />Hair spray<br />Cable ties</p><p>The one thing I haven&#039;t got is a dial gauge, I&#039;ve used paper and had fairly ok results. I don&#039;t believe things like motors, belts and pulleys are needed as spares, unless people have had problems with them in the past?</p><p>I&#039;d love to hear what you can&#039;t go without!</p>]]></content>
			<author>
				<name><![CDATA[pretenda]]></name>
				<uri>https://www.soliforum.com/user/231/</uri>
			</author>
			<updated>2013-07-16T13:39:07Z</updated>
			<id>https://www.soliforum.com/post/30000/#p30000</id>
		</entry>
</feed>