		<entry>
			<title type="html"><![CDATA[Re: Delamination w/ABS on a SD3 - what to do?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29940/#p29940" />
			<content type="html"><![CDATA[<p>Roger all that. Thanks, fellas.</p>]]></content>
			<author>
				<name><![CDATA[Heartlander]]></name>
				<uri>https://www.soliforum.com/user/2447/</uri>
			</author>
			<updated>2013-07-15T20:05:05Z</updated>
			<id>https://www.soliforum.com/post/29940/#p29940</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Delamination w/ABS on a SD3 - what to do?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29929/#p29929" />
			<content type="html"><![CDATA[<p>Give it a try. Might want to make sure you watch it closely for a while. As they show in their final test... things can melt if you don&#039;t pay attention. (IDK what they were doing using a thermometer that only went up to 120F)</p><p><a href="http://www.reptileuvinfo.com/html/watts-heat-lights-lamp-heat-output.html">http://www.reptileuvinfo.com/html/watts … utput.html</a></p>]]></content>
			<author>
				<name><![CDATA[2n2r5]]></name>
				<uri>https://www.soliforum.com/user/1906/</uri>
			</author>
			<updated>2013-07-15T18:16:26Z</updated>
			<id>https://www.soliforum.com/post/29929/#p29929</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Delamination w/ABS on a SD3 - what to do?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29926/#p29926" />
			<content type="html"><![CDATA[<p>I tried that once and nearly melted my extruder.&nbsp; The lamp needs to be pointed at something, which will probably get too hot.&nbsp; &nbsp;If you can find a way to aim it at the build plate and print without also hitting any of the printed components it might work.&nbsp; The air is more indirect and even. It comes in at about 70c and spreads out, averaging down to 45-50.&nbsp; &nbsp;If you want an alternative, I think a better one would be something like a heat pad in the bottom if the case with a gentle fan blowing over it.</p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2013-07-15T18:10:21Z</updated>
			<id>https://www.soliforum.com/post/29926/#p29926</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Delamination w/ABS on a SD3 - what to do?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29923/#p29923" />
			<content type="html"><![CDATA[<p>Nice work Ian. Do you think something like this would work too, a small heat lamp? Radiant heat instead of heated air?</p><p><span class="postimg"><img src="https://lh3.googleusercontent.com/public/bXD_w0M55aQqtT_QINqQ58p_6i4llYMTTI2kTpvXANkn7_znmyha3twGbUqzhAqZ17VUJiMmUcKJOpYBOnSO8Y9ayq0_k11WgNc7xQip7qe-R5PiGyG5RsM0K0IZE2a31NUt8cc6VjQ=s220-c" alt="https://lh3.googleusercontent.com/public/bXD_w0M55aQqtT_QINqQ58p_6i4llYMTTI2kTpvXANkn7_znmyha3twGbUqzhAqZ17VUJiMmUcKJOpYBOnSO8Y9ayq0_k11WgNc7xQip7qe-R5PiGyG5RsM0K0IZE2a31NUt8cc6VjQ=s220-c" /></span></p>]]></content>
			<author>
				<name><![CDATA[Heartlander]]></name>
				<uri>https://www.soliforum.com/user/2447/</uri>
			</author>
			<updated>2013-07-15T17:53:58Z</updated>
			<id>https://www.soliforum.com/post/29923/#p29923</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Delamination w/ABS on a SD3 - what to do?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29897/#p29897" />
			<content type="html"><![CDATA[<p>I find that lately the same print and filament produce perfect prints one day and fuzzy messes with nothing adhering at all the next day, depending on humidity.</p>]]></content>
			<author>
				<name><![CDATA[Hunter Green]]></name>
				<uri>https://www.soliforum.com/user/1356/</uri>
			</author>
			<updated>2013-07-15T11:05:15Z</updated>
			<id>https://www.soliforum.com/post/29897/#p29897</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Delamination w/ABS on a SD3 - what to do?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29887/#p29887" />
			<content type="html"><![CDATA[<p>Is it a tall part, or wide?&nbsp; More solid, thicker areas are actually more challenging because there is more plastic shrinking, creating more warping force.&nbsp; &nbsp;I heat the build area of my printer with this space heater - <a href="http://www.amazon.com/Lasko-100-MyHeat-Personal-Ceramic/dp/B003XDTWN2/ref=sr_1_1?ie=UTF8&amp;qid=1373863171&amp;sr=8-1&amp;keywords=personal+space+heater">http://www.amazon.com/Lasko-100-MyHeat- … ace+heater</a></p><p>It&#039;s only about 7&quot; tall, and I point it into a bit of 3&quot; duct leading into a case I made.&nbsp; If I have a print that I think is going to be a challenge due to being tall, or wide and flat, I&#039;ll run the heater for a few minutes before the print to warm up the air and inside surfaces.&nbsp; It gets to about 45C inside, which seems to be enough to prevent most problems.&nbsp; Make sure the air doesn&#039;t blow directly on the print, because moving air at 70C is still a cooling breeze</p><p><span class="postimg"><img src="http://thingiverse-production.s3.amazonaws.com/assets/c4/b5/be/e7/89/IMG_5910.JPG" alt="http://thingiverse-production.s3.amazonaws.com/assets/c4/b5/be/e7/89/IMG_5910.JPG" /></span></p><p><span class="postimg"><img src="http://thingiverse-production.s3.amazonaws.com/assets/7a/f3/f2/7d/0a/IMG_5913.JPG" alt="http://thingiverse-production.s3.amazonaws.com/assets/7a/f3/f2/7d/0a/IMG_5913.JPG" /></span></p><p><a href="http://www.thingiverse.com/thing:34754">http://www.thingiverse.com/thing:34754</a></p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2013-07-15T04:48:33Z</updated>
			<id>https://www.soliforum.com/post/29887/#p29887</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Delamination w/ABS on a SD3 - what to do?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29885/#p29885" />
			<content type="html"><![CDATA[<p>I&#039;m seeing layers separating on my part, even areas that are nice thick solids. I run the extruder at 195C, bed at 85C. No fan (yet). Covers on and closed. What am I doing wrong?</p>]]></content>
			<author>
				<name><![CDATA[Heartlander]]></name>
				<uri>https://www.soliforum.com/user/2447/</uri>
			</author>
			<updated>2013-07-15T04:04:32Z</updated>
			<id>https://www.soliforum.com/post/29885/#p29885</id>
		</entry>