<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Anyone using ABS pellets from carlsievering on eBay?]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/3164/" />
	<updated>2013-07-27T20:44:08Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/3164/anyone-using-abs-pellets-from-carlsievering-on-ebay/</id>
		<entry>
			<title type="html"><![CDATA[Re: Anyone using ABS pellets from carlsievering on eBay?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/31157/#p31157" />
			<content type="html"><![CDATA[<p>I printed a calibration angle with the grey. .3 mm layers on a printrbot with a .4mm nozzle. Bumped the temp up from 210 to 225.Green is ABS from matterhackers. I might have printed it at .2<br /><span class="postimg"><img src="http://imgur.com/VVKA5Ce" alt="http://imgur.com/VVKA5Ce" /></span></p>]]></content>
			<author>
				<name><![CDATA[Nimikin]]></name>
				<uri>https://www.soliforum.com/user/1533/</uri>
			</author>
			<updated>2013-07-27T20:44:08Z</updated>
			<id>https://www.soliforum.com/post/31157/#p31157</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Anyone using ABS pellets from carlsievering on eBay?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/31109/#p31109" />
			<content type="html"><![CDATA[<p>I&#039;ve been going for about 24 hours now on the white pellets, and have only extruded a pound or so. This last batch is looking pretty clean, so I am going to try printing it.</p>]]></content>
			<author>
				<name><![CDATA[Nimikin]]></name>
				<uri>https://www.soliforum.com/user/1533/</uri>
			</author>
			<updated>2013-07-27T04:45:39Z</updated>
			<id>https://www.soliforum.com/post/31109/#p31109</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Anyone using ABS pellets from carlsievering on eBay?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29768/#p29768" />
			<content type="html"><![CDATA[<p>I emded up with anout 10 lbs of the white and 18 lbs of the natural from him. I just got my shipping notice for my Filastruder yesterday though <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /> so I&#039;ll let you know.</p>]]></content>
			<author>
				<name><![CDATA[Nimikin]]></name>
				<uri>https://www.soliforum.com/user/1533/</uri>
			</author>
			<updated>2013-07-13T18:52:23Z</updated>
			<id>https://www.soliforum.com/post/29768/#p29768</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Anyone using ABS pellets from carlsievering on eBay?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29754/#p29754" />
			<content type="html"><![CDATA[<p>You could try bumping the temp up, but it sounds like the pellets you have have a pretty low MFI. You can also mix them 50/50 with higher MFI pellets, like MG94.</p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2013-07-13T16:51:18Z</updated>
			<id>https://www.soliforum.com/post/29754/#p29754</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Anyone using ABS pellets from carlsievering on eBay?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29752/#p29752" />
			<content type="html"><![CDATA[<p>Thanks. I guess I&#039;ll be making a lot of white or maybe some pale colors.&nbsp; I like the filament made from the pellets although the Filastruder really goes slow making it.</p>]]></content>
			<author>
				<name><![CDATA[jetpad]]></name>
				<uri>https://www.soliforum.com/user/2182/</uri>
			</author>
			<updated>2013-07-13T16:33:12Z</updated>
			<id>https://www.soliforum.com/post/29752/#p29752</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Anyone using ABS pellets from carlsievering on eBay?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29746/#p29746" />
			<content type="html"><![CDATA[<p>I bought one pound from Carl&#039;s ebay store.&nbsp; The problem is that white pellets contain white colorant, which is why your filament is coming out pink.&nbsp; Mixing ABS colorant is subtractive not additive.</p><p><a href="http://imgur.com/AIjiZ33"><span class="postimg"><img src="http://i.imgur.com/AIjiZ33.jpg" alt="http://i.imgur.com/AIjiZ33.jpg" /></span></a></p><p>You need natural (uncolored) ABS pellets to to make colored filament.</p>]]></content>
			<author>
				<name><![CDATA[jesse]]></name>
				<uri>https://www.soliforum.com/user/1984/</uri>
			</author>
			<updated>2013-07-13T15:58:46Z</updated>
			<id>https://www.soliforum.com/post/29746/#p29746</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Anyone using ABS pellets from carlsievering on eBay?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/29743/#p29743" />
			<content type="html"><![CDATA[<p>Anyone else using ABS pellets from carlsievering off of eBay? I&#039;d ordered it before OSPrinting had any available. I tried coloring it red but it came out pink. I&#039;d like to try making some black filament with it but I suspect it&#039;ll just come out grey. What should the ratio for it using the black master batch?</p>]]></content>
			<author>
				<name><![CDATA[jetpad]]></name>
				<uri>https://www.soliforum.com/user/2182/</uri>
			</author>
			<updated>2013-07-13T15:20:55Z</updated>
			<id>https://www.soliforum.com/post/29743/#p29743</id>
		</entry>
</feed>