<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — How to tell the difference between pla and abs?]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/285/" />
	<updated>2012-11-15T22:11:39Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/285/how-to-tell-the-difference-between-pla-and-abs/</id>
		<entry>
			<title type="html"><![CDATA[Re: How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/4712/#p4712" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>IanJohnson wrote:</cite><blockquote><p>I&#039;ve heard it just turns whitish and gets brittle.&nbsp; Everything that I&#039;ve seen mentioned that dissolves PLA is way more dangerous than acetone.&nbsp; You can use a lye/water solution to dissolve PLA completely when using it as support material.&nbsp; It might be possible to use that for smoothing, but I have a feeling it wouldn&#039;t be as fast or effective as acetone is with ABS.</p></blockquote></div><p>This is one potential advantage to sticking to ABS.</p>]]></content>
			<author>
				<name><![CDATA[solijohn]]></name>
				<uri>https://www.soliforum.com/user/7/</uri>
			</author>
			<updated>2012-11-15T22:11:39Z</updated>
			<id>https://www.soliforum.com/post/4712/#p4712</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/3904/#p3904" />
			<content type="html"><![CDATA[<p>I&#039;ve heard it just turns whitish and gets brittle.&nbsp; Everything that I&#039;ve seen mentioned that dissolves PLA is way more dangerous than acetone.&nbsp; You can use a lye/water solution to dissolve PLA completely when using it as support material.&nbsp; It might be possible to use that for smoothing, but I have a feeling it wouldn&#039;t be as fast or effective as acetone is with ABS.</p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2012-11-02T05:02:57Z</updated>
			<id>https://www.soliforum.com/post/3904/#p3904</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/3903/#p3903" />
			<content type="html"><![CDATA[<p>How does pla react to acetone?</p>]]></content>
			<author>
				<name><![CDATA[ch355ma5t3r]]></name>
				<uri>https://www.soliforum.com/user/161/</uri>
			</author>
			<updated>2012-11-02T04:50:07Z</updated>
			<id>https://www.soliforum.com/post/3903/#p3903</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2225/#p2225" />
			<content type="html"><![CDATA[<p>Ian, the color is yellow and it came from the the same supplier I got the clear from.&nbsp; This was one of the spools I didn&#039;t order but received due to a mix up.&nbsp; What I <em>think</em> happened was that it may have oozed back into the black plastic piece because the dia is only 1.62mm.</p>]]></content>
			<author>
				<name><![CDATA[ch355ma5t3r]]></name>
				<uri>https://www.soliforum.com/user/161/</uri>
			</author>
			<updated>2012-10-13T04:59:18Z</updated>
			<id>https://www.soliforum.com/post/2225/#p2225</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2163/#p2163" />
			<content type="html"><![CDATA[<p>Take my opinion for what its worth as I don&#039;t have a printer or any filament to truly know but could the filament be damp or have absorbed some moisture? Might need to dry it out a bit and try again</p>]]></content>
			<author>
				<name><![CDATA[devilman2075]]></name>
				<uri>https://www.soliforum.com/user/70/</uri>
			</author>
			<updated>2012-10-11T22:48:14Z</updated>
			<id>https://www.soliforum.com/post/2163/#p2163</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2133/#p2133" />
			<content type="html"><![CDATA[<p>Where did you get it, and what color?</p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2012-10-11T12:42:54Z</updated>
			<id>https://www.soliforum.com/post/2133/#p2133</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2130/#p2130" />
			<content type="html"><![CDATA[<p>Thank you for all the suggestions.&nbsp; The filament in question burns a bit more vigorously than some other abs I have and it bends easier.&nbsp; It smells pretty much the same when burnt so I think it is abs.&nbsp; It clogged up my hot end almost immediately and I&#039;ve been having a heck of a time getting it sorted out.&nbsp; Everything else I&#039;ve gotten from this particular supplier has been spot on so it&#039;s possible that something else may be the problem.&nbsp; If I figure it out I&#039;ll let you know.</p>]]></content>
			<author>
				<name><![CDATA[ch355ma5t3r]]></name>
				<uri>https://www.soliforum.com/user/161/</uri>
			</author>
			<updated>2012-10-11T08:14:22Z</updated>
			<id>https://www.soliforum.com/post/2130/#p2130</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2095/#p2095" />
			<content type="html"><![CDATA[<p>Easiest would be burning a little.&nbsp; Also PLA is stiffer than ABS.&nbsp; If you bend it, it will snap.&nbsp; ABS turns white when you bend it, and breaks after some fatigue.</p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2012-10-10T13:53:24Z</updated>
			<id>https://www.soliforum.com/post/2095/#p2095</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2092/#p2092" />
			<content type="html"><![CDATA[<p>Isn&#039;t PLA a lot more brittle as well?</p>]]></content>
			<author>
				<name><![CDATA[Donitz]]></name>
				<uri>https://www.soliforum.com/user/45/</uri>
			</author>
			<updated>2012-10-10T13:14:03Z</updated>
			<id>https://www.soliforum.com/post/2092/#p2092</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2089/#p2089" />
			<content type="html"><![CDATA[<p>PLA has a much lower melting point. Apply heat to known ABS at the same time and see if it melts significantly quicker.</p>]]></content>
			<author>
				<name><![CDATA[lawsy]]></name>
				<uri>https://www.soliforum.com/user/51/</uri>
			</author>
			<updated>2012-10-10T11:05:57Z</updated>
			<id>https://www.soliforum.com/post/2089/#p2089</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2088/#p2088" />
			<content type="html"><![CDATA[<p>put it in water and wait?&nbsp; &nbsp;the pla is biodegradable .. or try to burn it with a lighter.. the odor of pla is like popcorn...</p>]]></content>
			<author>
				<name><![CDATA[ysb]]></name>
				<uri>https://www.soliforum.com/user/40/</uri>
			</author>
			<updated>2012-10-10T10:19:28Z</updated>
			<id>https://www.soliforum.com/post/2088/#p2088</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[How to tell the difference between pla and abs?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2086/#p2086" />
			<content type="html"><![CDATA[<p>I have a new roll of filament that doesn&#039;t seem quite right.&nbsp; Is there a simple test to tell if it&#039;s pla or abs?</p>]]></content>
			<author>
				<name><![CDATA[ch355ma5t3r]]></name>
				<uri>https://www.soliforum.com/user/161/</uri>
			</author>
			<updated>2012-10-10T07:44:55Z</updated>
			<id>https://www.soliforum.com/post/2086/#p2086</id>
		</entry>
</feed>