			<title type="html"><![CDATA[Re: Filastruder plans?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/26765/#p26765" />
			<content type="html"><![CDATA[<p>Never mind.&nbsp; I found another thread that explained the futility of trying.&nbsp; Not that I wont try at a later date.</p>]]></content>
			<author>
				<name><![CDATA[Downeasta]]></name>
				<uri>https://www.soliforum.com/user/2351/</uri>
			</author>
			<updated>2013-06-18T01:50:30Z</updated>
			<id>https://www.soliforum.com/post/26765/#p26765</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Filastruder plans?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/26651/#p26651" />
			<content type="html"><![CDATA[<p>Hey downeasta, If you are looking to maybe build or design one yourself most people start with lymans design <a href="http://www.thingiverse.com/thing:30642">http://www.thingiverse.com/thing:30642</a> and go from there, there are lots of specs in the notes.</p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2013-06-17T06:27:34Z</updated>
			<id>https://www.soliforum.com/post/26651/#p26651</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Filastruder plans?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/26635/#p26635" />
			<content type="html"><![CDATA[<p>Downeasta,</p><p>There are no design documents published, only assembly and operation. Many of the parts are prohibitively expensive to buy in single unit quantities.</p><p>Your best best is to email filastruder@gmail.com to get on the wait list - you&#039;ll be notified as soon as one is ready to be ordered/shipped. It might be sooner than Solidoodle delivers your printer. <img src="https://www.soliforum.com/img/smilies/wink.png" width="15" height="15" alt="wink" /></p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2013-06-17T04:08:41Z</updated>
			<id>https://www.soliforum.com/post/26635/#p26635</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Filastruder plans?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/26633/#p26633" />
			<content type="html"><![CDATA[<p>Does anyone have blueprints of making one of these?&nbsp; Yes I have seen some of the youtube postings stating to use a 0.75&quot; wood auger in a tube with some form of heater on the end.</p><p>Yet I need better info, like:<br />-rpms of auger.<br />-amount of torque required<br />-does a larger auger work better than a small one?<br />-or is a smaller auger better?<br />-heater build</p>]]></content>
			<author>
				<name><![CDATA[Downeasta]]></name>
				<uri>https://www.soliforum.com/user/2351/</uri>
			</author>
			<updated>2013-06-17T03:34:44Z</updated>
			<id>https://www.soliforum.com/post/26633/#p26633</id>
		</entry>
</feed>