<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Print quality with white ABS]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/2806/" />
	<updated>2013-06-14T20:20:04Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/2806/print-quality-with-white-abs/</id>
		<entry>
			<title type="html"><![CDATA[Re: Print quality with white ABS]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/26381/#p26381" />
			<content type="html"><![CDATA[<p>From a search for &quot;oven&quot;, second link:</p><p><a href="http://www.soliforum.com/post/25993/#p25993">http://www.soliforum.com/post/25993/#p25993</a></p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2013-06-14T20:20:04Z</updated>
			<id>https://www.soliforum.com/post/26381/#p26381</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Print quality with white ABS]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/26373/#p26373" />
			<content type="html"><![CDATA[<p>Thanks for your quick response.</p><p>How long do you recommend baking a standard spool?</p>]]></content>
			<author>
				<name><![CDATA[dlemmink]]></name>
				<uri>https://www.soliforum.com/user/119/</uri>
			</author>
			<updated>2013-06-14T19:17:07Z</updated>
			<id>https://www.soliforum.com/post/26373/#p26373</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Print quality with white ABS]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/26368/#p26368" />
			<content type="html"><![CDATA[<p>Rough surface is usually moisture, dry that spool of filament in the oven at 190F or so.</p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2013-06-14T18:54:56Z</updated>
			<id>https://www.soliforum.com/post/26368/#p26368</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Print quality with white ABS]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/26363/#p26363" />
			<content type="html"><![CDATA[<p>I seem to have problems with print quality when using white ABS.&nbsp; Prints end up with as splotchy rough surface.&nbsp; Can someone help me and determine if it&#039;s just a bad reel of ABS, or a temperature/flowrate issue.</p><p>This is printed on a SD2 @ 200degrees. </p><p> I&#039;ve tried altering the feedrates with no improvement.</p>]]></content>
			<author>
				<name><![CDATA[dlemmink]]></name>
				<uri>https://www.soliforum.com/user/119/</uri>
			</author>
			<updated>2013-06-14T18:06:52Z</updated>
			<id>https://www.soliforum.com/post/26363/#p26363</id>
		</entry>
</feed>