<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — is there a printer sleep function?]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/280/" />
	<updated>2012-10-31T14:01:48Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/280/is-there-a-printer-sleep-function/</id>
		<entry>
			<title type="html"><![CDATA[Re: is there a printer sleep function?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/3738/#p3738" />
			<content type="html"><![CDATA[<p>So add this to the end of the gcode?</p>]]></content>
			<author>
				<name><![CDATA[utt.josh]]></name>
				<uri>https://www.soliforum.com/user/303/</uri>
			</author>
			<updated>2012-10-31T14:01:48Z</updated>
			<id>https://www.soliforum.com/post/3738/#p3738</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: is there a printer sleep function?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2290/#p2290" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>lawsy wrote:</cite><blockquote><p>M104 S0 ; kill extruder temperature<br />M140 S0 ; kill bed temperature<br />M84 ; disable motors</p></blockquote></div><p>Perfect!&nbsp; Just in time for a print-and-sleep tonight.</p>]]></content>
			<author>
				<name><![CDATA[driggers]]></name>
				<uri>https://www.soliforum.com/user/211/</uri>
			</author>
			<updated>2012-10-15T08:03:38Z</updated>
			<id>https://www.soliforum.com/post/2290/#p2290</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: is there a printer sleep function?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2053/#p2053" />
			<content type="html"><![CDATA[<p>M104 S0 ; kill extruder temperature<br />M140 S0 ; kill bed temperature<br />M84 ; disable motors</p>]]></content>
			<author>
				<name><![CDATA[lawsy]]></name>
				<uri>https://www.soliforum.com/user/51/</uri>
			</author>
			<updated>2012-10-08T10:18:53Z</updated>
			<id>https://www.soliforum.com/post/2053/#p2053</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[is there a printer sleep function?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/2048/#p2048" />
			<content type="html"><![CDATA[<p>Does the software have a sleep function which would turn the heaters off after a print is finished?</p>]]></content>
			<author>
				<name><![CDATA[driggers]]></name>
				<uri>https://www.soliforum.com/user/211/</uri>
			</author>
			<updated>2012-10-08T06:20:33Z</updated>
			<id>https://www.soliforum.com/post/2048/#p2048</id>
		</entry>
</feed>