	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Printing at .1mm, I'm getting some holes in the top of my prints]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/262/" />
	<updated>2012-10-03T15:57:15Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/262/printing-at-1mm-im-getting-some-holes-in-the-top-of-my-prints/</id>
		<entry>
			<title type="html"><![CDATA[Re: Printing at .1mm, I'm getting some holes in the top of my prints]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/1933/#p1933" />
			<content type="html"><![CDATA[<p>It&#039;s called Honeycomb in Slic3r.</p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2012-10-03T15:57:15Z</updated>
			<id>https://www.soliforum.com/post/1933/#p1933</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Printing at .1mm, I'm getting some holes in the top of my prints]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/1928/#p1928" />
			<content type="html"><![CDATA[<p>Ian,</p><p>I&#039;ve got the width set to .42 I think already (I&#039;m not at the printer right now to check.&nbsp; The holes are in the top of the model.&nbsp; Can we set the infill to hexagonal in Slic3r?&nbsp; I thought that was only for support material not infill.&nbsp; Anyway I will have a look when I get back to the printer tonight.</p>]]></content>
			<author>
				<name><![CDATA[JustSomeGuyTN]]></name>
				<uri>https://www.soliforum.com/user/96/</uri>
			</author>
			<updated>2012-10-03T15:21:01Z</updated>
			<id>https://www.soliforum.com/post/1928/#p1928</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Printing at .1mm, I'm getting some holes in the top of my prints]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/1922/#p1922" />
			<content type="html"><![CDATA[<p>Are the holes on the flat top of the print, or is there a curved edge (fillet) leading to the top?&nbsp; If the holes are on the edge, you need more perimeters.&nbsp; If the holes are on the top, you need more infill or maybe 1-2 extra solid layers.&nbsp; A hexagonal infill will support a top layer better than something like Line.</p><p>You can also set the thread widths to .42 rather than leaving them at 0, which is automatic.&nbsp; A wider thread will be able to support a layer above that is set way back due to a shallow curve.</p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2012-10-03T13:56:17Z</updated>
			<id>https://www.soliforum.com/post/1922/#p1922</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Printing at .1mm, I'm getting some holes in the top of my prints]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/1920/#p1920" />
			<content type="html"><![CDATA[<p>I&#039;m getting some holes in the tops of my prints.&nbsp; I&#039;m printing at .1mm layer height with infill on each layer at .20 density.&nbsp; Oh, and I&#039;m using Slic3r and&nbsp; Repetier.&nbsp; I will try to post a picture later.&nbsp; Does anyone have a suggestion for what to tweak settings wise?&nbsp; I was thinking I might need to set the perimeters higher.&nbsp; I&#039;m not sure what it&#039;s set to now.&nbsp; Probably the default.</p>]]></content>
			<author>
				<name><![CDATA[JustSomeGuyTN]]></name>
				<uri>https://www.soliforum.com/user/96/</uri>
			</author>
			<updated>2012-10-03T13:31:09Z</updated>
			<id>https://www.soliforum.com/post/1920/#p1920</id>
		</entry>
</feed>