<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Unexpected printing stop]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/250/" />
	<updated>2014-04-03T03:02:34Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/250/unexpected-printing-stop/</id>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/53419/#p53419" />
			<content type="html"><![CDATA[<p>Having the exact same problem. Have my printer for over 8 months now. I recently changed extruder because of&nbsp; a clog. Been printing fine for 2 weeks and then it started happening. Just randomly stops printing. Sometimes will disconnect after 3 hours, or as soon as 2 minutes. It re ally is random.</p><p>So for the past 8 months I have had none of this problem and it just started happening last week. Didnt check stepper motor temperature yet, but as the printer stopped in the very begining i suspect its not related. Didnt notice anything from other things on and off in the apartment, maybe its the neighbors fault XD. Its not sleep as it happens as i would be using the computer, and its not something else in the computer as i tested with recently restarted and nothing other then CURA open. Tested with RH and Cura with diferent settings and its still happening EVERYTIME at very random times.</p><p>Will continue to investigate as I need this printer running ASAP.<br />Using MacOS Lion. Standard USB cable and no mods in the printer.and im testing with the exact same STL everytime. And i already printed it several times before.</p>]]></content>
			<author>
				<name><![CDATA[Ryuudan]]></name>
				<uri>https://www.soliforum.com/user/5423/</uri>
			</author>
			<updated>2014-04-03T03:02:34Z</updated>
			<id>https://www.soliforum.com/post/53419/#p53419</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/52459/#p52459" />
			<content type="html"><![CDATA[<p>Yep I had the same last night.&nbsp; It has failed before and I have re-soldered the connections a couple of times but now it&#039;s just time to upgrade.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-03-19T01:19:34Z</updated>
			<id>https://www.soliforum.com/post/52459/#p52459</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/52458/#p52458" />
			<content type="html"><![CDATA[<p>Really?&nbsp; I would have thought there&#039;d be other indications, like not being able to heat things to temperature or whatnot. I don&#039;t even need to power cycle to get things working again, I just have to disconnect and close RH, unplug he USB cable from the computer, plug it back in, fire up RH, and everything works again.</p>]]></content>
			<author>
				<name><![CDATA[Skyminer]]></name>
				<uri>https://www.soliforum.com/user/4607/</uri>
			</author>
			<updated>2014-03-19T01:16:11Z</updated>
			<id>https://www.soliforum.com/post/52458/#p52458</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/52454/#p52454" />
			<content type="html"><![CDATA[<p>I wouldn&#039;t be surprised at all.&nbsp; My power supply failed last night and that is exactly what happens.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-03-19T01:10:54Z</updated>
			<id>https://www.soliforum.com/post/52454/#p52454</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/52453/#p52453" />
			<content type="html"><![CDATA[<p>I have the same issue with stopping mid print occasionally. It wouldn&#039;t be so bad if when it happened it turned the extruder heater off, but it doesn&#039;t. The nozzle just sits there, presumably cooking ABS. </p><p>I can&#039;t trace the stoppages back to anything in particular.. Ie lights, stove, etc. it just seems random. Solidoodle support has advised me to return my power supply for exchange, but I&#039;d really be surprised if that fixed the problem.</p>]]></content>
			<author>
				<name><![CDATA[Skyminer]]></name>
				<uri>https://www.soliforum.com/user/4607/</uri>
			</author>
			<updated>2014-03-19T01:02:54Z</updated>
			<id>https://www.soliforum.com/post/52453/#p52453</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/52430/#p52430" />
			<content type="html"><![CDATA[<p>+ 1 on the power spikes, i have had a few prints ruined by the printer stopping midt print because i turned lights/oven on og off.</p>]]></content>
			<author>
				<name><![CDATA[CarstenBe]]></name>
				<uri>https://www.soliforum.com/user/4901/</uri>
			</author>
			<updated>2014-03-18T18:44:03Z</updated>
			<id>https://www.soliforum.com/post/52430/#p52430</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/51322/#p51322" />
			<content type="html"><![CDATA[<p>The USB connection can be suspect, which was what my cause was.&nbsp; I was using the supplied cable from Solidoodle, but I had it plugged into the front USB.&nbsp; I switched it to one on the back directly on the motherboard and I haven&#039;t had trouble since.</p><p>I&#039;m glad you were able to fix your issue as well!</p>]]></content>
			<author>
				<name><![CDATA[accusedmonk]]></name>
				<uri>https://www.soliforum.com/user/3772/</uri>
			</author>
			<updated>2014-03-03T05:56:36Z</updated>
			<id>https://www.soliforum.com/post/51322/#p51322</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/51315/#p51315" />
			<content type="html"><![CDATA[<p>I will try that next. Thanks again for the assistance.</p>]]></content>
			<author>
				<name><![CDATA[gushino]]></name>
				<uri>https://www.soliforum.com/user/4394/</uri>
			</author>
			<updated>2014-03-03T03:33:28Z</updated>
			<id>https://www.soliforum.com/post/51315/#p51315</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/51314/#p51314" />
			<content type="html"><![CDATA[<p>The red and blue ones for the heat cartridge and thermistor.&nbsp; I did replace them all... of course not much of my printer is original at this point.&nbsp; I do feel that it is important to have everything working properly before I will do a modification.&nbsp; This way when something doesn&#039;t work I can only blame myself <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-03-03T03:30:26Z</updated>
			<id>https://www.soliforum.com/post/51314/#p51314</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/51313/#p51313" />
			<content type="html"><![CDATA[<p>Thanks for your input wardjr. I will try your heat sink suggestion tomorrow. Which connections seem to be troublesome to you? Did you replace them?</p>]]></content>
			<author>
				<name><![CDATA[gushino]]></name>
				<uri>https://www.soliforum.com/user/4394/</uri>
			</author>
			<updated>2014-03-03T03:21:08Z</updated>
			<id>https://www.soliforum.com/post/51313/#p51313</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/51312/#p51312" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>gushino wrote:</cite><blockquote><p>wardjr,</p><p>Were you having the same stoppage problem that we have been having with our printers? And if so, did the heat sink solve the issue for you?</p></blockquote></div><p>No but once I enclosed the printer I had some skipping and it fixed that.&nbsp; I haven&#039;t really followed your thread but my guess would be a loose connection even though you have checked all of that stuff.&nbsp; Those connectors are not the best and were a constant source of frustration for me.&nbsp; Go find an old PC and steal a heat sink that is about the right size.&nbsp; What do you have to loose?</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-03-03T03:13:42Z</updated>
			<id>https://www.soliforum.com/post/51312/#p51312</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/51311/#p51311" />
			<content type="html"><![CDATA[<p>wardjr,</p><p>Were you having the same stoppage problem that we have been having with our printers? And if so, did the heat sink solve the issue for you?</p>]]></content>
			<author>
				<name><![CDATA[gushino]]></name>
				<uri>https://www.soliforum.com/user/4394/</uri>
			</author>
			<updated>2014-03-03T02:50:22Z</updated>
			<id>https://www.soliforum.com/post/51311/#p51311</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/51309/#p51309" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>gushino wrote:</cite><blockquote><p>The Y axis motor is not under enough of a load difference to compared to the X axis motor to justify a much smaller over heating over loaded motor. I would think that this would have showed up in testing, especially during burn in. At least a light weight heat sink and fan should have been added is all I&#039;m saying IMHPO.</p></blockquote></div><p>I agree 100%&nbsp; the first mod I ever did to my printer was to add a heat sink to that motor.&nbsp; I often think I should add a fan but the heat sink that I pulled off an old PC processor has just worked so well.&nbsp; I will say that a little extra mass can really screw up the ability to print at faster speeds.&nbsp; I certainly can tell the difference of the Bulldog XL&#039;s extra mass vs. the original extruder.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-03-03T02:42:13Z</updated>
			<id>https://www.soliforum.com/post/51309/#p51309</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/51307/#p51307" />
			<content type="html"><![CDATA[<p>The Y axis motor is not under enough of a load difference to compared to the X axis motor to justify a much smaller over heating over loaded motor. I would think that this would have showed up in testing, especially during burn in. At least a light weight heat sink and fan should have been added is all I&#039;m saying IMHPO.</p><p>In addition, I think that the fact that this is happening a lot now, almost every print in the last 2 days, that the motor is beginning to burn out.</p>]]></content>
			<author>
				<name><![CDATA[gushino]]></name>
				<uri>https://www.soliforum.com/user/4394/</uri>
			</author>
			<updated>2014-03-03T02:35:55Z</updated>
			<id>https://www.soliforum.com/post/51307/#p51307</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Unexpected printing stop]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/51306/#p51306" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>gushino wrote:</cite><blockquote><p>By the way, why is the X axis motor so small compare to all the other motors on the Solidoodle? This seems odd and unnecessary. When I design robotics, I try to keep everything uniform for ease of maintenance and consistency of performance. It is obviously being over loaded compared to the other larger motors.</p></blockquote></div><p>It could be bigger but you must consider the additional mass that would then become an additional load for the Y-motor.&nbsp; It&#039;s really a compromise of weight, torque and speed.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2014-03-03T02:15:19Z</updated>
			<id>https://www.soliforum.com/post/51306/#p51306</id>
		</entry>
</feed>