			<title type="html"><![CDATA[Re: First prints. Need some tips for adjustment to correct print errors.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/23171/#p23171" />
			<content type="html"><![CDATA[<p>I run the extrusion multiplier in Slic3r&nbsp; at 60% , prints text pretty good now.</p>]]></content>
			<author>
				<name><![CDATA[satman49]]></name>
				<uri>https://www.soliforum.com/user/574/</uri>
			</author>
			<updated>2013-05-18T04:17:30Z</updated>
			<id>https://www.soliforum.com/post/23171/#p23171</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: First prints. Need some tips for adjustment to correct print errors.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/23138/#p23138" />
			<content type="html"><![CDATA[<p>My SD3 overextruded about 30%.</p><br /><p>//Matte</p>]]></content>
			<author>
				<name><![CDATA[impulze]]></name>
				<uri>https://www.soliforum.com/user/1093/</uri>
			</author>
			<updated>2013-05-17T20:00:24Z</updated>
			<id>https://www.soliforum.com/post/23138/#p23138</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: First prints. Need some tips for adjustment to correct print errors.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/23123/#p23123" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>Stevos758 wrote:</cite><blockquote><p>I should do this first.</p><p><a href="http://www.youtube.com/watch?v=JZGdMc2ebPo&amp;w=560&amp;h=315">http://www.youtube.com/watch?v=JZGdMc2e … &amp;h=315</a></p></blockquote></div><p>Yes, definitely do that and I thought I put this link in my other post but must have forgot to paste it <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /> <a href="http://wiki.solidoodle.com/gettingstarted">http://wiki.solidoodle.com/gettingstarted</a></p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2013-05-17T16:42:16Z</updated>
			<id>https://www.soliforum.com/post/23123/#p23123</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: First prints. Need some tips for adjustment to correct print errors.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/23121/#p23121" />
			<content type="html"><![CDATA[<p>I should do this first.</p><p><a href="http://www.youtube.com/watch?v=JZGdMc2ebPo&amp;w=560&amp;h=315">http://www.youtube.com/watch?v=JZGdMc2e … &amp;h=315</a></p>]]></content>
			<author>
				<name><![CDATA[Stevos758]]></name>
				<uri>https://www.soliforum.com/user/1682/</uri>
			</author>
			<updated>2013-05-17T16:33:38Z</updated>
			<id>https://www.soliforum.com/post/23121/#p23121</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: First prints. Need some tips for adjustment to correct print errors.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/23117/#p23117" />
			<content type="html"><![CDATA[<p>Ok. So should I do this? I was going to try this out tonight.</p><p><a href="http://wiki.solidoodle.com/flow-rate">http://wiki.solidoodle.com/flow-rate</a></p>]]></content>
			<author>
				<name><![CDATA[Stevos758]]></name>
				<uri>https://www.soliforum.com/user/1682/</uri>
			</author>
			<updated>2013-05-17T16:25:43Z</updated>
			<id>https://www.soliforum.com/post/23117/#p23117</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: First prints. Need some tips for adjustment to correct print errors.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/23116/#p23116" />
			<content type="html"><![CDATA[<p>Looks like overextrusion is the biggest thing.</p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2013-05-17T16:19:43Z</updated>
			<id>https://www.soliforum.com/post/23116/#p23116</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: First prints. Need some tips for adjustment to correct print errors.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/23115/#p23115" />
			<content type="html"><![CDATA[<p>SD3. </p><p>I turned it on. Leveled the bed and adjusted the Z stop and started printing. That is all I have done so far. Just got it last night.</p>]]></content>
			<author>
				<name><![CDATA[Stevos758]]></name>
				<uri>https://www.soliforum.com/user/1682/</uri>
			</author>
			<updated>2013-05-17T16:10:53Z</updated>
			<id>https://www.soliforum.com/post/23115/#p23115</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: First prints. Need some tips for adjustment to correct print errors.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/23114/#p23114" />
			<content type="html"><![CDATA[<p>How much calibration have you done? <br />Is this an SD3?</p><p>//Matte</p>]]></content>
			<author>
				<name><![CDATA[impulze]]></name>
				<uri>https://www.soliforum.com/user/1093/</uri>
			</author>
			<updated>2013-05-17T16:09:14Z</updated>
			<id>https://www.soliforum.com/post/23114/#p23114</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: First prints. Need some tips for adjustment to correct print errors.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/23113/#p23113" />
			<content type="html"><![CDATA[<p>ABS</p>]]></content>
			<author>
				<name><![CDATA[Stevos758]]></name>
				<uri>https://www.soliforum.com/user/1682/</uri>
			</author>
			<updated>2013-05-17T15:59:25Z</updated>
			<id>https://www.soliforum.com/post/23113/#p23113</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: First prints. Need some tips for adjustment to correct print errors.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/23112/#p23112" />
			<content type="html"><![CDATA[<p>Is this ABS or PLA?</p><p>//Matte</p>]]></content>
			<author>
				<name><![CDATA[impulze]]></name>
				<uri>https://www.soliforum.com/user/1093/</uri>
			</author>
			<updated>2013-05-17T15:58:51Z</updated>
			<id>https://www.soliforum.com/post/23112/#p23112</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[First prints. Need some tips for adjustment to correct print errors.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/23106/#p23106" />
			<content type="html"><![CDATA[<p>Can someone help me and tell me how to fix these problems. </p><p>Pic 1 you can see it looks as if the nozzel was pushing into the model. I slowed down the feedrate and adjusted the z home slightly. It seemed to help.</p><p>Pic 2 you can see some distortion in my second print on th right. 25x25mm test cube. What is causing this distortion.<br />On the right of pic #2 there is the line down the side of the object. Should I chose random start point to get rid of this?</p><p>Pic3 Merica cookie cutter didn&#039;t work out so well. How do i fix this? More perimeters?</p><p>Pic 5 you can see the top layer is a little distorted. also my ends were curled a little. I&#039;m thinking an enclosure and fan will help?</p><p>Please be harsh and judge my first prints. Tell me what I am doing wrong/how to improve.</p><p>I plan to add an enclosure.<br />Fix the Z slop.<br />add cooling fan.</p>]]></content>
			<author>
				<name><![CDATA[Stevos758]]></name>
				<uri>https://www.soliforum.com/user/1682/</uri>
			</author>
			<updated>2013-05-17T14:23:23Z</updated>
			<id>https://www.soliforum.com/post/23106/#p23106</id>
		</entry>
</feed>