<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — What to inspect when receiving your Solidoodle?]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/243/" />
	<updated>2012-09-29T19:32:44Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/243/what-to-inspect-when-receiving-your-solidoodle/</id>
		<entry>
			<title type="html"><![CDATA[Re: What to inspect when receiving your Solidoodle?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/1774/#p1774" />
			<content type="html"><![CDATA[<p>skype or facetime is your best bet!&nbsp; <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /> At the very least text pics</p>]]></content>
			<author>
				<name><![CDATA[jooshs]]></name>
				<uri>https://www.soliforum.com/user/13/</uri>
			</author>
			<updated>2012-09-29T19:32:44Z</updated>
			<id>https://www.soliforum.com/post/1774/#p1774</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: What to inspect when receiving your Solidoodle?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/1773/#p1773" />
			<content type="html"><![CDATA[<p>Thanks guys, now I just have to figure out how to relay this information to someone who has difficulty turning the TV on.... I&#039;m thinking pictures with arrows are my best bet.</p>]]></content>
			<author>
				<name><![CDATA[Jason]]></name>
				<uri>https://www.soliforum.com/user/26/</uri>
			</author>
			<updated>2012-09-29T19:29:38Z</updated>
			<id>https://www.soliforum.com/post/1773/#p1773</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: What to inspect when receiving your Solidoodle?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/1771/#p1771" />
			<content type="html"><![CDATA[<p>She could look for cracks in the printed Y carriages, which ride on the rods on each side of the printer.</p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2012-09-29T19:07:20Z</updated>
			<id>https://www.soliforum.com/post/1771/#p1771</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: What to inspect when receiving your Solidoodle?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/1769/#p1769" />
			<content type="html"><![CDATA[<p>Really the only thing I see that might get damaged would be the electronics on the back of the unit.&nbsp; They are packaged pretty well though so removing all the bubble wrap carefully would be your best bet.&nbsp; The electronics are the only thing that aren&#039;t protected by the steel housing.</p>]]></content>
			<author>
				<name><![CDATA[ch355ma5t3r]]></name>
				<uri>https://www.soliforum.com/user/161/</uri>
			</author>
			<updated>2012-09-29T18:25:42Z</updated>
			<id>https://www.soliforum.com/post/1769/#p1769</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[What to inspect when receiving your Solidoodle?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/1739/#p1739" />
			<content type="html"><![CDATA[<p>I am away on business in the Middle East for a few months and my Solidoodle came in the mail right after I left (of course).&nbsp; My concern is that so much time will pass between when I received the printer and when I am home and able to inspect it for shipping damage that Solidoodle support may wonder why I am only now emailing them about shipping damage. </p><p>My fiance is available to remove my printer from the box and take pictures for me to inspect....&nbsp; What are the common parts that can be damaged in shipping?&nbsp; Also any tips to not damage the printer when removing packaging would help as well.</p><br /><p>Any help would be greatly appreciated!</p>]]></content>
			<author>
				<name><![CDATA[Jason]]></name>
				<uri>https://www.soliforum.com/user/26/</uri>
			</author>
			<updated>2012-09-29T03:42:58Z</updated>
			<id>https://www.soliforum.com/post/1739/#p1739</id>
		</entry>
</feed>