			<title type="html"><![CDATA[Re: Filastruder Temperature reading is incorrect]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/154825/#p154825" />
			<content type="html"><![CDATA[<p>How are you measuring the temperature with your multimeter? A photo might help.</p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2021-06-08T12:52:16Z</updated>
			<id>https://www.soliforum.com/post/154825/#p154825</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Filastruder Temperature reading is incorrect]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/154824/#p154824" />
			<content type="html"><![CDATA[<p>after running it a few times, total run time of a few hours, the temperature now reads only about 10 deg C higher than the actual temperature.&nbsp; &nbsp;Is that normal?</p><p>Thanks</p>]]></content>
			<author>
				<name><![CDATA[Mad Engineer]]></name>
				<uri>https://www.soliforum.com/user/25762/</uri>
			</author>
			<updated>2021-06-07T22:46:36Z</updated>
			<id>https://www.soliforum.com/post/154824/#p154824</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Filastruder Temperature reading is incorrect]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/154821/#p154821" />
			<content type="html"><![CDATA[<p>I just calibrated my PID controller, and everything looked good, but when I compared temps with a 2nd temperature sensor, the filastruder temp was reading 40deg higher than the temp reading from my multi-meter.&nbsp; is there any way to calibrate the temp reading on the filastruder PID?</p><p>Thanks</p>]]></content>
			<author>
				<name><![CDATA[Mad Engineer]]></name>
				<uri>https://www.soliforum.com/user/25762/</uri>
			</author>
			<updated>2021-06-07T13:50:00Z</updated>
			<id>https://www.soliforum.com/post/154821/#p154821</id>
		</entry>
</feed>