<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Nylon and glass filled filament Questions]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/18537/" />
	<updated>2020-04-16T23:18:16Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/18537/nylon-and-glass-filled-filament-questions/</id>
		<entry>
			<title type="html"><![CDATA[Nylon and glass filled filament Questions]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/153037/#p153037" />
			<content type="html"><![CDATA[<p>So i just got my filastruder and I plan on extruding 33% glass fiber nylon. I know that it will wear out my nozzle and thats ok. I plan on wire EDMing a tungsten or hardend steel nozzle. Has anyone been extruding nylon, and nylon with glass in it? Just curious.</p>]]></content>
			<author>
				<name><![CDATA[slistack]]></name>
				<uri>https://www.soliforum.com/user/24107/</uri>
			</author>
			<updated>2020-04-16T23:18:16Z</updated>
			<id>https://www.soliforum.com/post/153037/#p153037</id>
		</entry>
</feed>