<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Are the fumes from printing with ABS toxic?]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/1824/" />
	<updated>2013-03-23T18:09:34Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/1824/are-the-fumes-from-printing-with-abs-toxic/</id>
		<entry>
			<title type="html"><![CDATA[Re: Are the fumes from printing with ABS toxic?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/17431/#p17431" />
			<content type="html"><![CDATA[<p>Great, thanks for the reply.&nbsp; Good to know my 3d printer won&#039;t give me cancer or something. <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p>]]></content>
			<author>
				<name><![CDATA[lazzy_8]]></name>
				<uri>https://www.soliforum.com/user/990/</uri>
			</author>
			<updated>2013-03-23T18:09:34Z</updated>
			<id>https://www.soliforum.com/post/17431/#p17431</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Are the fumes from printing with ABS toxic?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/17426/#p17426" />
			<content type="html"><![CDATA[<p>I run mine with an enclosure, vented through a window with a 80mm case fan.</p><p>ABS starts offgassing HCN and CO at about 350C, and really starts offgassing around 600C. Normal printing temperatures are around 200C, so you should be safe from dangerous fumes, but the smell makes some people uncomfortable. It&#039;s kinda like painting - a good idea to do it in a well-ventilated area, but not likely to kill you or give you more than a headache.</p>]]></content>
			<author>
				<name><![CDATA[elmoret]]></name>
				<uri>https://www.soliforum.com/user/221/</uri>
			</author>
			<updated>2013-03-23T18:03:54Z</updated>
			<id>https://www.soliforum.com/post/17426/#p17426</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Are the fumes from printing with ABS toxic?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/17421/#p17421" />
			<content type="html"><![CDATA[<p>I&#039;m in a room with my new printer printing away and I&#039;ve noticed the place filling up with the smell of burnt plastic.&nbsp; Should I not operate this device in a closed room?&nbsp; Are the fumes dangerous?&nbsp; Is it safter if I were to build an enclosure so the fumes wouldn&#039;t leak out as much?</p>]]></content>
			<author>
				<name><![CDATA[lazzy_8]]></name>
				<uri>https://www.soliforum.com/user/990/</uri>
			</author>
			<updated>2013-03-23T17:20:20Z</updated>
			<id>https://www.soliforum.com/post/17421/#p17421</id>
		</entry>
</feed>