<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Best filament resources for Europe?]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/1719/" />
	<updated>2019-01-30T06:53:58Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/1719/best-filament-resources-for-europe/</id>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/148758/#p148758" />
			<content type="html"><![CDATA[<p>TIANSE is currently public 3D printer filament supplier. They provide quality 3d filament. With this type of filament you will never have to worry about prints failing. You also get reel replacement guarantee which means you can buy filament without any risk.</p><p>Contact: <a href="http://www.tianseoffice.com">www.tianseoffice.com</a><br />Mail: sales@tianseoffice.com</p>]]></content>
			<author>
				<name><![CDATA[esteel]]></name>
				<uri>https://www.soliforum.com/user/20987/</uri>
			</author>
			<updated>2019-01-30T06:53:58Z</updated>
			<id>https://www.soliforum.com/post/148758/#p148758</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/122394/#p122394" />
			<content type="html"><![CDATA[<p>If you need some good quality filamets of one producer in EU.<br />Contact: <a href="http://www.azurefilm.com">www.azurefilm.com</a><br />Mail: info@azurefilm.com</p><p>Best Regards,<br />Jure Derman</p>]]></content>
			<author>
				<name><![CDATA[zuroj.d]]></name>
				<uri>https://www.soliforum.com/user/14371/</uri>
			</author>
			<updated>2016-05-06T21:00:12Z</updated>
			<id>https://www.soliforum.com/post/122394/#p122394</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96573/#p96573" />
			<content type="html"><![CDATA[<p>Full disclosure, I represent the company linked. We do cater to the entire European market though. We ship our filament from Dublin, Ireland.</p><p><a href="http://www.Ink3D.ie">www.Ink3D.ie</a> </p><p>If anyone has any questions I&#039;d be happy to answer them.</p><p>Best,</p><p>David Pigot.<br />Sales Manager | Ink3D.ie<br />+353-(86)-1513629 | info@ink3d.ie | <a href="http://www.ink3d.ie">www.ink3d.ie</a> | Twitter: @InkThreeD | Facebook: <a href="http://www.facebook.com/ink3d.ie">www.facebook.com/ink3d.ie</a> |</p><p>EDIT: The reason this may be of particular interest to European 3D printer users is that there is free shipping for all European orders.</p>]]></content>
			<author>
				<name><![CDATA[Ink3D.ie]]></name>
				<uri>https://www.soliforum.com/user/10890/</uri>
			</author>
			<updated>2015-05-21T14:55:51Z</updated>
			<id>https://www.soliforum.com/post/96573/#p96573</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/59337/#p59337" />
			<content type="html"><![CDATA[<p>We sale 3d filament oversea<br />Cheack [redacted].com</p>]]></content>
			<author>
				<name><![CDATA[jpson]]></name>
				<uri>https://www.soliforum.com/user/4427/</uri>
			</author>
			<updated>2014-06-26T02:06:06Z</updated>
			<id>https://www.soliforum.com/post/59337/#p59337</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/58704/#p58704" />
			<content type="html"><![CDATA[<p>THe extra charge from overseas is not much as long as you got cheap price.</p><p>Check for 3Dfilamenta.com</p>]]></content>
			<author>
				<name><![CDATA[oklok]]></name>
				<uri>https://www.soliforum.com/user/6232/</uri>
			</author>
			<updated>2014-06-16T00:19:15Z</updated>
			<id>https://www.soliforum.com/post/58704/#p58704</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/56919/#p56919" />
			<content type="html"><![CDATA[<p>hello, maybe you can order some filament from Internet, for instance:&nbsp; aliexpress.com<br />very convenient and good price, good quality filament offfer on this website. we usually buy filaments and parts from this website.</p>]]></content>
			<author>
				<name><![CDATA[liuzehu]]></name>
				<uri>https://www.soliforum.com/user/5975/</uri>
			</author>
			<updated>2014-05-24T05:39:57Z</updated>
			<id>https://www.soliforum.com/post/56919/#p56919</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/56586/#p56586" />
			<content type="html"><![CDATA[<p>Although my advice is a bit too late, I can recommend igo3d.com <br />The ABS filament works quite well with the Solidoodle, they are based in Germany, and their 6x 1kg roll for 120€ including shipping is great bang for the buck.</p>]]></content>
			<author>
				<name><![CDATA[agentsmith]]></name>
				<uri>https://www.soliforum.com/user/2336/</uri>
			</author>
			<updated>2014-05-19T18:46:48Z</updated>
			<id>https://www.soliforum.com/post/56586/#p56586</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/55706/#p55706" />
			<content type="html"><![CDATA[<p>3dprima.com<br />works really good accros whole Europe</p>]]></content>
			<author>
				<name><![CDATA[jaco]]></name>
				<uri>https://www.soliforum.com/user/5790/</uri>
			</author>
			<updated>2014-05-05T18:38:57Z</updated>
			<id>https://www.soliforum.com/post/55706/#p55706</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/26262/#p26262" />
			<content type="html"><![CDATA[<p>I&#039;ve struggled getting the extrusion temperature hot enough for formfortura yellow and blue. White, green and black worked fine</p>]]></content>
			<author>
				<name><![CDATA[Staffordknot]]></name>
				<uri>https://www.soliforum.com/user/1769/</uri>
			</author>
			<updated>2013-06-13T20:51:29Z</updated>
			<id>https://www.soliforum.com/post/26262/#p26262</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/26204/#p26204" />
			<content type="html"><![CDATA[<p>Formfutura.com would be my recommendation!</p>]]></content>
			<author>
				<name><![CDATA[3Dprintergear]]></name>
				<uri>https://www.soliforum.com/user/80/</uri>
			</author>
			<updated>2013-06-13T09:44:26Z</updated>
			<id>https://www.soliforum.com/post/26204/#p26204</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/17833/#p17833" />
			<content type="html"><![CDATA[<p>I usually order the filaments from here SainSmart</p><p>They have free shipping to usa and for other countries, it&#039;s only $5. Maybe this is what you want.</p>]]></content>
			<author>
				<name><![CDATA[mansfieldpark]]></name>
				<uri>https://www.soliforum.com/user/1106/</uri>
			</author>
			<updated>2013-03-27T01:58:35Z</updated>
			<id>https://www.soliforum.com/post/17833/#p17833</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/16810/#p16810" />
			<content type="html"><![CDATA[<p>RainBot3D was really good to me and I think he will ship there.</p><p>link: <a href="https://rainbot3d.com/">https://rainbot3d.com/</a> also on ebay as rainbot3d</p>]]></content>
			<author>
				<name><![CDATA[frozensoda]]></name>
				<uri>https://www.soliforum.com/user/738/</uri>
			</author>
			<updated>2013-03-18T10:06:44Z</updated>
			<id>https://www.soliforum.com/post/16810/#p16810</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/16809/#p16809" />
			<content type="html"><![CDATA[<p>Check ebay, there are some dealers in UK.</p><p>//Matte</p>]]></content>
			<author>
				<name><![CDATA[impulze]]></name>
				<uri>https://www.soliforum.com/user/1093/</uri>
			</author>
			<updated>2013-03-18T09:21:47Z</updated>
			<id>https://www.soliforum.com/post/16809/#p16809</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/16456/#p16456" />
			<content type="html"><![CDATA[<p><a href="http://fabber-parts.de/shop/">http://fabber-parts.de/shop/</a></p><p>But I have a warning ... please read my thread :<br /><a href="http://www.soliforum.com/topic/1705/pla-temperature-problem/">http://www.soliforum.com/topic/1705/pla … e-problem/</a></p>]]></content>
			<author>
				<name><![CDATA[Kvirre]]></name>
				<uri>https://www.soliforum.com/user/207/</uri>
			</author>
			<updated>2013-03-14T13:16:53Z</updated>
			<id>https://www.soliforum.com/post/16456/#p16456</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Best filament resources for Europe?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/16454/#p16454" />
			<content type="html"><![CDATA[<p>Hi </p><p>I am quite new to the 3D printing. I got my Solidoodle&nbsp; last week and ordered some filament direct from Solidoodle.</p><p>As importing to Europe is quite expensive due to customs and shipping I&#039;m wondering if there are good resources for filament fitting my Solidoodle. I am located in Germany but will order anywhere in Europe as long as I can avoid these overseas extra charges.</p><p>Thanks for suggestions</p><p>Elias</p>]]></content>
			<author>
				<name><![CDATA[elias]]></name>
				<uri>https://www.soliforum.com/user/1226/</uri>
			</author>
			<updated>2013-03-14T13:10:14Z</updated>
			<id>https://www.soliforum.com/post/16454/#p16454</id>
		</entry>
</feed>