<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — A new-to-me way to adjust for filament diameter variation]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/1702/" />
	<updated>2013-03-13T17:11:29Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/1702/a-newtome-way-to-adjust-for-filament-diameter-variation/</id>
		<entry>
			<title type="html"><![CDATA[Re: A new-to-me way to adjust for filament diameter variation]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/16328/#p16328" />
			<content type="html"><![CDATA[<p>I like your idea Teal, nice and simple... I am leaning more toward the electronic solution though... that way I can factor in the &#039;delay&#039; filament length offset.</p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2013-03-13T17:11:29Z</updated>
			<id>https://www.soliforum.com/post/16328/#p16328</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: A new-to-me way to adjust for filament diameter variation]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/16309/#p16309" />
			<content type="html"><![CDATA[<p>Interesting.&nbsp; Seems like a good idea, but I&#039;m wondering if it would be possible for an extruder to adjust its speed automatically, at least for a course adjustment.&nbsp; I&#039;m thinking of a cone-shaped drive gear along with a pair of grooved wheels that size the filament; something like this (excuse the crappy drawing):</p><p><span class="postimg"><img src="http://www.soliforum.com/misc.php?action=pun_attachment&amp;item=1457" alt="http://www.soliforum.com/misc.php?action=pun_attachment&amp;amp;item=1457" /></span></p>]]></content>
			<author>
				<name><![CDATA[tealvince]]></name>
				<uri>https://www.soliforum.com/user/676/</uri>
			</author>
			<updated>2013-03-13T15:53:03Z</updated>
			<id>https://www.soliforum.com/post/16309/#p16309</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[A new-to-me way to adjust for filament diameter variation]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/16272/#p16272" />
			<content type="html"><![CDATA[<p>This posting is worth a look.</p><p><a href="https://groups.google.com/forum/?fromgroups=#!topic/trinitylabs-talk/Mu79M8tNsbY">https://groups.google.com/forum/?fromgr … u79M8tNsbY</a></p><p>Triffid Hunter&#039;s approach was new to me, and seems easy to implement, and flexible.</p>]]></content>
			<author>
				<name><![CDATA[jon_bondy]]></name>
				<uri>https://www.soliforum.com/user/181/</uri>
			</author>
			<updated>2013-03-13T12:04:53Z</updated>
			<id>https://www.soliforum.com/post/16272/#p16272</id>
		</entry>