			<title type="html"><![CDATA[Re: [ASA] - Geloy CR7500]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/157272/#p157272" />
			<content type="html"><![CDATA[<p>Hello Mr. Preston,</p><p>I am interested in ASA filament for my industrial 3d printer. I believe that it should made from Geloy CR7500.<br />Original filament ASA is working good.<br />Temperature of Tip (nozzle) for ASA on 3d printer =340 °C (not open for regulation)<br />I tested 3 other filament producers. And all of them clog the Tip quickly.</p><p>Coud you tell me what Tip temperature did you use on 3d printer for filament ASA Geloy CR7500?</p>]]></content>
			<author>
				<name><![CDATA[abvhot@gmail.com]]></name>
				<uri>https://www.soliforum.com/user/27917/</uri>
			</author>
			<updated>2025-07-15T17:29:11Z</updated>
			<id>https://www.soliforum.com/post/157272/#p157272</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[[ASA] - Geloy CR7500]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/135738/#p135738" />
			<content type="html"><![CDATA[<p>I wanted to try ASA filament because of Thomas Sanladerer&#039;s filaween video. I only found two different types of ASA pellets on ebay, ASA TW-23V&nbsp; and ASA GELOY CR7500. I went with ASA GELOY CR7500 since the TW-23V had a really low melt flow rate.</p><p><span class="bbu"><strong>Extruder:</strong> </span><br /><strong>Nozzle Diameter:</strong> 1.6mm<br />A vertical Filastruder v2.0 #2690 with a filawinder<br /><span class="postimg"><img src="http://soliforum.com/i/?rTzCXHy.jpg" alt="http://soliforum.com/i/?rTzCXHy.jpg" /></span></p><p><span class="bbu"><strong>Drying:</strong></span><br />I always dry my pellets before use. I used a toaster oven at 70°C for about 6 hours. The image shows the pellets on the tray after drying.<br /><span class="postimg"><img src="http://soliforum.com/i/?iSUCFHt.jpg" alt="http://soliforum.com/i/?iSUCFHt.jpg" /></span></p><p><span class="bbu"><strong>Extrusion:</strong></span><br /><strong>Temperature:</strong> 195°C<br /><strong>Extrusion Rate:</strong> 4-5&quot; per minute<br /><strong>Average diameter:</strong> 1.76 +/- 0.02mm<br /><span class="postimg"><img src="http://soliforum.com/i/?G9Oq14L.jpg" alt="http://soliforum.com/i/?G9Oq14L.jpg" /></span></p><p><span class="bbu"><strong>Printer:</strong></span><br />Robo 3D R1 Plus, E3D v6, Hardened steel 0.4mm nozzle, acrylic enclosure</p><p><span class="bbu"><strong>Prints:</strong></span><br /><strong>Temperature:</strong> 240°C/80°C<br /><strong>Speed:</strong> 50mm/s<br /><strong>Layer height: </strong>0.2mm<br /><strong>Infill:</strong> 25%<br /><strong>Fan speed:</strong> 25%</p><p>3D Benchy<br /><span class="postimg"><img src="http://soliforum.com/i/?ureyuCv.jpg" alt="http://soliforum.com/i/?ureyuCv.jpg" /></span><br />Make magazine test<br /><span class="postimg"><img src="http://soliforum.com/i/?qJy4OT5.jpg" alt="http://soliforum.com/i/?qJy4OT5.jpg" /></span></p><p><span class="bbu"><strong>Comparison to available filament:</strong></span><br />I&#039;ve never bought ASA filament before, so I cant really compare this to anything. It seems to do small details and overhangs better than ABS, but it&#039;s layer adhesion is pretty weak. I might try printing with the temp up more.</p><p><span class="bbu"><strong>Takeaway and comments:</strong></span><br />The extrusion was really slow and there weren&#039;t really any benefits to this over ABS. The diameter was really consistent though and there weren&#039;t much fumes. I probably won&#039;t be getting any more of this unless I can get the print quality better.</p>]]></content>
			<author>
				<name><![CDATA[Preston]]></name>
				<uri>https://www.soliforum.com/user/15691/</uri>
			</author>
			<updated>2017-05-30T08:11:12Z</updated>
			<id>https://www.soliforum.com/post/135738/#p135738</id>
		</entry>
</feed>