			<title type="html"><![CDATA[Re: from 1.75 to 3 mm]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/128672/#p128672" />
			<content type="html"><![CDATA[<p>if you get the new style cartridge thermistors, they come with a connector on a short pigtail, then all you need is the other side of that connector to run to the controller board... </p><p>then all you would have to do is figure out a way to connect the heater cartridge wires... the XT-30 RC battery connectors are quite nice for that aspect of things... small enough to not get in the way, but plenty sturdy enough for the application. <img src="https://www.soliforum.com/img/smilies/wink.png" width="15" height="15" alt="wink" /> just a simple matter of snipping the wires at a convenient location and soldering in the connectors.</p>]]></content>
			<author>
				<name><![CDATA[heartless]]></name>
				<uri>https://www.soliforum.com/user/10399/</uri>
			</author>
			<updated>2016-12-03T00:03:01Z</updated>
			<id>https://www.soliforum.com/post/128672/#p128672</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: from 1.75 to 3 mm]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/128670/#p128670" />
			<content type="html"><![CDATA[<p>no need to change the fan or the heater block. <br />Tin</p>]]></content>
			<author>
				<name><![CDATA[Tin Falcon]]></name>
				<uri>https://www.soliforum.com/user/6775/</uri>
			</author>
			<updated>2016-12-02T23:51:16Z</updated>
			<id>https://www.soliforum.com/post/128670/#p128670</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: from 1.75 to 3 mm]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/128656/#p128656" />
			<content type="html"><![CDATA[<p>Thanks that what&nbsp; I was thinking, anyway the lite version is cheap, so I&#039;m gonna do that.</p><p>I just need to figure out a system to switch plug and play the heater fan and termistor ....</p>]]></content>
			<author>
				<name><![CDATA[sigiel]]></name>
				<uri>https://www.soliforum.com/user/2977/</uri>
			</author>
			<updated>2016-12-02T15:46:23Z</updated>
			<id>https://www.soliforum.com/post/128656/#p128656</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: from 1.75 to 3 mm]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/128651/#p128651" />
			<content type="html"><![CDATA[<p>i believe the heatsink is different as well, not just the heatbreak (threaded part)<br />they may look the same on the outside, but the internal drilling is done differently between the two</p>]]></content>
			<author>
				<name><![CDATA[heartless]]></name>
				<uri>https://www.soliforum.com/user/10399/</uri>
			</author>
			<updated>2016-12-02T12:43:26Z</updated>
			<id>https://www.soliforum.com/post/128651/#p128651</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: from 1.75 to 3 mm]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/128650/#p128650" />
			<content type="html"><![CDATA[<p>IIRC the heat break need to be changed so no without ordering the needed parts to change the ED3 </p><br /><br /><p>Hopefully one of the experts will clarify this.</p>]]></content>
			<author>
				<name><![CDATA[Tin Falcon]]></name>
				<uri>https://www.soliforum.com/user/6775/</uri>
			</author>
			<updated>2016-12-02T11:49:42Z</updated>
			<id>https://www.soliforum.com/post/128650/#p128650</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[from 1.75 to 3 mm]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/128649/#p128649" />
			<content type="html"><![CDATA[<p>hi</p><p>I have the edv6 1.75 and by mistake i bought 2 rollsl of 3mm filament (no turnng back)</p><p>I noticed that the diameter of the extruder was bigger. can i change the PTFE tubing and use the 3mm filament ? <br />on a temp basis.</p><p>thanks you.</p>]]></content>
			<author>
				<name><![CDATA[sigiel]]></name>
				<uri>https://www.soliforum.com/user/2977/</uri>
			</author>
			<updated>2016-12-02T08:37:30Z</updated>
			<id>https://www.soliforum.com/post/128649/#p128649</id>