		<entry>
			<title type="html"><![CDATA[Re: HELP! Repetier-Printer Connection Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/14940/#p14940" />
			<content type="html"><![CDATA[<p>If you have a digital camera or cel phone to take pics of the extruder there are plenty of us on here that can spot problems and help you out <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2013-03-04T06:02:18Z</updated>
			<id>https://www.soliforum.com/post/14940/#p14940</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: HELP! Repetier-Printer Connection Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/14939/#p14939" />
			<content type="html"><![CDATA[<p>UPDATE: a new USB cable and using another port did the trick. Now to determine why the extruder is not feeding the filament correctly upon starting a job. :S</p><p>I&#039;ll get it...</p><p>Thanks for helping a noobie out!</p>]]></content>
			<author>
				<name><![CDATA[paulwiedemeier]]></name>
				<uri>https://www.soliforum.com/user/1065/</uri>
			</author>
			<updated>2013-03-04T05:55:37Z</updated>
			<id>https://www.soliforum.com/post/14939/#p14939</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: HELP! Repetier-Printer Connection Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/14910/#p14910" />
			<content type="html"><![CDATA[<p>It would not allow me to insert the text into the forum submission so i&#039;ve uploaded it as a .txt file here.</p><p>I&#039;m pretty darn sure I&#039;ve got the right port. Would the communicating Baud rate of that port be an issue? My COM3 seems to be running at about 56000 whereas the printer settings show a COM3 port Baud at 250000...</p>]]></content>
			<author>
				<name><![CDATA[paulwiedemeier]]></name>
				<uri>https://www.soliforum.com/user/1065/</uri>
			</author>
			<updated>2013-03-03T22:27:44Z</updated>
			<id>https://www.soliforum.com/post/14910/#p14910</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: HELP! Repetier-Printer Connection Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/14909/#p14909" />
			<content type="html"><![CDATA[<p>When you click on the &#039;Connect&#039; button (top left of the screen) does any thing show up in the bottom window? like error messages, status, etc...</p>]]></content>
			<author>
				<name><![CDATA[ronsii]]></name>
				<uri>https://www.soliforum.com/user/296/</uri>
			</author>
			<updated>2013-03-03T22:20:05Z</updated>
			<id>https://www.soliforum.com/post/14909/#p14909</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: HELP! Repetier-Printer Connection Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/14907/#p14907" />
			<content type="html"><![CDATA[<p>Your connection-button is labeled &quot;Disconnect&quot;.<br />Your printer should make some &quot;noise&quot; if you connect and disconnect. <br />Sorry for the &quot;silly&quot; questions because I had the same problem but the problem was no problem.<br />I just had the wrong Com-Port. You double-checked the virual-com-port in the device-manager (if you are running on windows)</p>]]></content>
			<author>
				<name><![CDATA[digiprint]]></name>
				<uri>https://www.soliforum.com/user/364/</uri>
			</author>
			<updated>2013-03-03T22:05:22Z</updated>
			<id>https://www.soliforum.com/post/14907/#p14907</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: HELP! Repetier-Printer Connection Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/14904/#p14904" />
			<content type="html"><![CDATA[<p>Yes my COM3. And yes. There is also this &#039;Virtual Printer&#039; dropdown option on the printer settings. I&#039;m assuming this is some sort of &#039;dry run&#039; type setting.</p>]]></content>
			<author>
				<name><![CDATA[paulwiedemeier]]></name>
				<uri>https://www.soliforum.com/user/1065/</uri>
			</author>
			<updated>2013-03-03T21:55:39Z</updated>
			<id>https://www.soliforum.com/post/14904/#p14904</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: HELP! Repetier-Printer Connection Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/14903/#p14903" />
			<content type="html"><![CDATA[<p>Do you select the right COM-port?<br />Are you connected to the printer?</p>]]></content>
			<author>
				<name><![CDATA[digiprint]]></name>
				<uri>https://www.soliforum.com/user/364/</uri>
			</author>
			<updated>2013-03-03T21:54:04Z</updated>
			<id>https://www.soliforum.com/post/14903/#p14903</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[HELP! Repetier-Printer Connection Issues]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/14901/#p14901" />
			<content type="html"><![CDATA[<p>Just received my SD2 and began downloading the software pactages found on the How-To page. So after plugging everything in, I&#039;ve downloaded Repetier V0.82 and updated my USB Serial Converter &amp; Port drivers to the latest (1/18/13) releases yet I am still having &#039;connection&#039; issues. </p><p>I can load an STL file, manipulate it, slice it, and see the Gcode. Where I&#039;m running into problems is getting the printer to respond to the Manual Control tab. I can&#039;t move the extruder along the XYZ axis or heat the extruder to pull the factory filament out. :S</p><p>Has anyone else had the problems or have an idea on how to troubleshoot?</p>]]></content>
			<author>
				<name><![CDATA[paulwiedemeier]]></name>