<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — parts extruder help]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/13669/" />
	<updated>2016-02-21T11:57:57Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/13669/parts-extruder-help/</id>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/117101/#p117101" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>scobo wrote:</cite><blockquote><p>I removed it as I&#039;ve no use for it anymore.<br />Makes things much tidier. <img src="https://www.soliforum.com/img/smilies/wink.png" width="15" height="15" alt="wink" /></p></blockquote></div><p>I almost finished <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p><p>for termistor you use the red and black cable that goes into the pcb of the original extruder DaVinci?</p><br /><p>here <a href="http://www.soliforum.com/post/90407/#p90407">http://www.soliforum.com/post/90407/#p90407</a> :</p><p><strong>thermistor (no polarity): black and yellow&nbsp; &nbsp;???</strong>&nbsp; I am confused</p><br /><br /><br /><p>thx help</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2016-02-21T11:57:57Z</updated>
			<id>https://www.soliforum.com/post/117101/#p117101</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/117100/#p117100" />
			<content type="html"><![CDATA[<p>I removed it as I&#039;ve no use for it anymore.<br />Makes things much tidier. <img src="https://www.soliforum.com/img/smilies/wink.png" width="15" height="15" alt="wink" /></p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-21T10:57:48Z</updated>
			<id>https://www.soliforum.com/post/117100/#p117100</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/117099/#p117099" />
			<content type="html"><![CDATA[<p>scobo,<br />you use the electronic pcb of the extruder DaVinci?<br />youtube <a href="https://www.youtube.com/watch?v=m-xatvqd3aU">https://www.youtube.com/watch?v=m-xatvqd3aU</a> it means in use.<br />thx help</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2016-02-21T10:54:34Z</updated>
			<id>https://www.soliforum.com/post/117099/#p117099</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/117023/#p117023" />
			<content type="html"><![CDATA[<p>I guess you could tap into 12v on the board but I just use an external 12v supply.<br />That way I can turn it on/off manually.<br />You need to have the fan all the time when printing or you run the risk of a jam.<br />I only turn the fan off while the extruder is getting up to temp to save time then switch it on as soon as the print starts.</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-20T07:53:55Z</updated>
			<id>https://www.soliforum.com/post/117023/#p117023</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/117008/#p117008" />
			<content type="html"><![CDATA[<p>hello scobo...</p><p>you use the 12V on the DaVinci pcb ? you can stop the fan by the simplefy3d program?<br />printer for the ABS stop the fan I pose?</p><p>thx</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2016-02-19T23:29:00Z</updated>
			<id>https://www.soliforum.com/post/117008/#p117008</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116646/#p116646" />
			<content type="html"><![CDATA[<p>Yeah, PLA will be fine for that.<br />I made a similar one with PLA. It helps a lot with small prints.</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-16T14:45:57Z</updated>
			<id>https://www.soliforum.com/post/116646/#p116646</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116633/#p116633" />
			<content type="html"><![CDATA[<p>ok thank you I just ordered <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /><br />this <a href="http://www.thingiverse.com/thing:822476">http://www.thingiverse.com/thing:822476</a> you not use pla ?</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2016-02-16T13:26:00Z</updated>
			<id>https://www.soliforum.com/post/116633/#p116633</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116627/#p116627" />
			<content type="html"><![CDATA[<p>The E3D&#039;s come with a fan and duct. <br />The stock fan is too big and won&#039;t fit.</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-16T12:32:57Z</updated>
			<id>https://www.soliforum.com/post/116627/#p116627</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116626/#p116626" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>scobo wrote:</cite><blockquote><p>Here&#039;s a few pics of my E3D v6 Lite setup ......</p><br /><p><span class="postimg"><img src="http://i882.photobucket.com/albums/ac28/scobodon/ac96acbdc73d9dc2475ad0235e16d3c9_zps8h0w9ufx.jpg" alt="http://i882.photobucket.com/albums/ac28/scobodon/ac96acbdc73d9dc2475ad0235e16d3c9_zps8h0w9ufx.jpg" /></span></p><br /><p><span class="postimg"><img src="http://i882.photobucket.com/albums/ac28/scobodon/886281dac6c27cba77252ab989c655ea_zpsuz0iknve.jpg" alt="http://i882.photobucket.com/albums/ac28/scobodon/886281dac6c27cba77252ab989c655ea_zpsuz0iknve.jpg" /></span></p><br /><p><span class="postimg"><img src="http://i882.photobucket.com/albums/ac28/scobodon/e271f3468f5a551962f2ae30c64216a9_zpsqvhthy7q.jpg" alt="http://i882.photobucket.com/albums/ac28/scobodon/e271f3468f5a551962f2ae30c64216a9_zpsqvhthy7q.jpg" /></span></p></blockquote></div><p>I see that you add a fan, it came with the parts e3d lite or is the fan of DaVinci?</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2016-02-16T12:28:26Z</updated>
			<id>https://www.soliforum.com/post/116626/#p116626</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116591/#p116591" />
			<content type="html"><![CDATA[<p>thx man</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2016-02-15T22:47:46Z</updated>
			<id>https://www.soliforum.com/post/116591/#p116591</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116579/#p116579" />
			<content type="html"><![CDATA[<p>Here&#039;s a few pics of my E3D v6 Lite setup ......</p><br /><p><span class="postimg"><img src="http://i882.photobucket.com/albums/ac28/scobodon/ac96acbdc73d9dc2475ad0235e16d3c9_zps8h0w9ufx.jpg" alt="http://i882.photobucket.com/albums/ac28/scobodon/ac96acbdc73d9dc2475ad0235e16d3c9_zps8h0w9ufx.jpg" /></span></p><br /><p><span class="postimg"><img src="http://i882.photobucket.com/albums/ac28/scobodon/886281dac6c27cba77252ab989c655ea_zpsuz0iknve.jpg" alt="http://i882.photobucket.com/albums/ac28/scobodon/886281dac6c27cba77252ab989c655ea_zpsuz0iknve.jpg" /></span></p><br /><p><span class="postimg"><img src="http://i882.photobucket.com/albums/ac28/scobodon/e271f3468f5a551962f2ae30c64216a9_zpsqvhthy7q.jpg" alt="http://i882.photobucket.com/albums/ac28/scobodon/e271f3468f5a551962f2ae30c64216a9_zpsqvhthy7q.jpg" /></span></p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-15T20:26:23Z</updated>
			<id>https://www.soliforum.com/post/116579/#p116579</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116577/#p116577" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>custom.made wrote:</cite><blockquote><p>Your in the EU? You can buy a new extruder from Da Vinci for about 70 EUR. Or contact them directly to see who your local supplier are. They told me that where I purchased it from should sell them but when I replied they didn&#039;t. They game me the UK reseller that does. So you can order parts its just question as to if you have to have the whole thing. I imagine theyll sell you a heater block though.</p></blockquote></div><p>ok i have send mail service ...</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2016-02-15T20:12:13Z</updated>
			<id>https://www.soliforum.com/post/116577/#p116577</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116568/#p116568" />
			<content type="html"><![CDATA[<p>Your in the EU? You can buy a new extruder from Da Vinci for about 70 EUR. Or contact them directly to see who your local supplier are. They told me that where I purchased it from should sell them but when I replied they didn&#039;t. They game me the UK reseller that does. So you can order parts its just question as to if you have to have the whole thing. I imagine theyll sell you a heater block though.</p>]]></content>
			<author>
				<name><![CDATA[custom.made]]></name>
				<uri>https://www.soliforum.com/user/12285/</uri>
			</author>
			<updated>2016-02-15T18:45:36Z</updated>
			<id>https://www.soliforum.com/post/116568/#p116568</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116564/#p116564" />
			<content type="html"><![CDATA[<p>It&#039;s up to you but the bowden version will require a different setup.<br />The direct drive version is the one described in the youtube video and is easier to install.</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-15T18:23:38Z</updated>
			<id>https://www.soliforum.com/post/116564/#p116564</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: parts extruder help]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116561/#p116561" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>scobo wrote:</cite><blockquote><p><a href="http://e3d-online.com/Lite6">http://e3d-online.com/Lite6</a><br />There&#039;s a guide to installation on the site.<br />The Lite is cheaper than the standard E3D but it&#039;s limited to 240C.<br />I can post a pic of my setup later.</p></blockquote></div><p>hello</p><p><a href="http://e3d-online.com/Lite6-1.75mm-Universal">http://e3d-online.com/Lite6-1.75mm-Universal</a><br />or<br /><a href="http://e3d-online.com/Lite6-1.75mm-Bowden">http://e3d-online.com/Lite6-1.75mm-Bowden</a></p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2016-02-15T17:52:57Z</updated>
			<id>https://www.soliforum.com/post/116561/#p116561</id>
		</entry>
</feed>