	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Acrylic bed ?]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/13656/" />
	<updated>2016-02-23T08:07:56Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/13656/acrylic-bed/</id>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/117304/#p117304" />
			<content type="html"><![CDATA[<p>The panel is 4mm thickness.<br />I didn&#039;t make any z adjustement, I just lowered the bed manually with the adjusters.<br />I use four 40mm bulldog clips. The one at the far right needs to go in front of the bed adjuster or the nozzle will slam into it.</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-23T08:07:56Z</updated>
			<id>https://www.soliforum.com/post/117304/#p117304</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/117302/#p117302" />
			<content type="html"><![CDATA[<p>The acrylic is quite thick.&nbsp; &nbsp;The stuff I have is much thinner.&nbsp; Hopefully that won&#039;t warp more.</p><p>Did you make your z adjustment in the printer settings or with g code?</p><p>How many clips?</p>]]></content>
			<author>
				<name><![CDATA[Telemachus]]></name>
				<uri>https://www.soliforum.com/user/13355/</uri>
			</author>
			<updated>2016-02-23T07:47:17Z</updated>
			<id>https://www.soliforum.com/post/117302/#p117302</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/117300/#p117300" />
			<content type="html"><![CDATA[<p>Thanks. <br />Not bad for 0.3mm layer height.</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-23T07:18:10Z</updated>
			<id>https://www.soliforum.com/post/117300/#p117300</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/117297/#p117297" />
			<content type="html"><![CDATA[<p>Beautiful!</p>]]></content>
			<author>
				<name><![CDATA[Telemachus]]></name>
				<uri>https://www.soliforum.com/user/13355/</uri>
			</author>
			<updated>2016-02-23T06:51:51Z</updated>
			<id>https://www.soliforum.com/post/117297/#p117297</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/117046/#p117046" />
			<content type="html"><![CDATA[<p>This is one of the biggest prints I&#039;ve done so far, covers about 80% of the bed.<br />Printed with wood-based filament which adhered to the acrylic/hairspray great ..... </p><p><span class="postimg"><img src="http://i882.photobucket.com/albums/ac28/scobodon/698b7cb5c454b79424e9859e7a0f6113_zpslaj1bpic.jpg" alt="http://i882.photobucket.com/albums/ac28/scobodon/698b7cb5c454b79424e9859e7a0f6113_zpslaj1bpic.jpg" /></span></p><p><span class="postimg"><img src="http://i882.photobucket.com/albums/ac28/scobodon/4502e54e4846479674eb1928ef04e14a_zpsrkaryn9c.jpg" alt="http://i882.photobucket.com/albums/ac28/scobodon/4502e54e4846479674eb1928ef04e14a_zpsrkaryn9c.jpg" /></span></p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-20T18:53:45Z</updated>
			<id>https://www.soliforum.com/post/117046/#p117046</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116654/#p116654" />
			<content type="html"><![CDATA[<p>So far, I&#039;ve tried up to 60°C and it seems fine.<br />With hairspray, I doubt you&#039;d need to go much higher as ABS and PLA seem to stick very well at that temp.<br />I tried a print last night that covered about a third of the bed and there was no warping at all.</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-16T16:10:33Z</updated>
			<id>https://www.soliforum.com/post/116654/#p116654</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116651/#p116651" />
			<content type="html"><![CDATA[<p>So what bed temp for ABS with acrylic?&nbsp; How about warping on larger prints?</p>]]></content>
			<author>
				<name><![CDATA[Telemachus]]></name>
				<uri>https://www.soliforum.com/user/13355/</uri>
			</author>
			<updated>2016-02-16T15:48:35Z</updated>
			<id>https://www.soliforum.com/post/116651/#p116651</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116580/#p116580" />
			<content type="html"><![CDATA[<p>Ok, I just had a go with some (very cheap) hairspray on the acrylic sheet and it works REALLY well !<br />ABS and PLA both really easy to remove and excellent adhesion. <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /><br />Reckon I&#039;ll be using this from now on.</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-15T20:33:00Z</updated>
			<id>https://www.soliforum.com/post/116580/#p116580</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116563/#p116563" />
			<content type="html"><![CDATA[<p>Just to update, haven&#039;t tried hairspray yet but securing the plate with bulldogclips has fixed the curling/warping issue so I can now set the bed hotter if I need to.<br />Must say, It&#039;s very handy having a removable plate. So much easier to clean and remove prints from.</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-15T17:55:10Z</updated>
			<id>https://www.soliforum.com/post/116563/#p116563</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116529/#p116529" />
			<content type="html"><![CDATA[<p>It might be a nice way to make a clear bottom on a pla print...</p>]]></content>
			<author>
				<name><![CDATA[Telemachus]]></name>
				<uri>https://www.soliforum.com/user/13355/</uri>
			</author>
			<updated>2016-02-15T05:21:32Z</updated>
			<id>https://www.soliforum.com/post/116529/#p116529</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116476/#p116476" />
			<content type="html"><![CDATA[<p>Cheers. I may give it a go later. The panel only cost £3 so no big deal if it goes wrong.</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-14T08:30:45Z</updated>
			<id>https://www.soliforum.com/post/116476/#p116476</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116474/#p116474" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>scobo wrote:</cite><blockquote><p>Yeah the acrylic. Sorry, should have made that clearer.<br />Carl, would PLA work with hairspray on acrylic or would it still fuse ?</p></blockquote></div><p>Can&#039;t answer that one, never tried..</p><br /><p>I just know there is some sort of reaction between PLA and acrylic at the temps that we use that make the PLA seem to be glues to the acrylic. They might as well be one piece.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2016-02-14T07:53:07Z</updated>
			<id>https://www.soliforum.com/post/116474/#p116474</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116473/#p116473" />
			<content type="html"><![CDATA[<p>Yeah the acrylic. Sorry, should have made that clearer.<br />Carl, would PLA work with hairspray on acrylic or would it still fuse ?</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-02-14T07:43:49Z</updated>
			<id>https://www.soliforum.com/post/116473/#p116473</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116459/#p116459" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>Telemachus wrote:</cite><blockquote><p>The acrylic curls or the print?</p></blockquote></div><br /><p>The acrylic curls....</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2016-02-14T02:16:14Z</updated>
			<id>https://www.soliforum.com/post/116459/#p116459</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Acrylic bed ?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/116457/#p116457" />
			<content type="html"><![CDATA[<p>The acrylic curls or the print?</p>]]></content>
			<author>
				<name><![CDATA[Telemachus]]></name>
				<uri>https://www.soliforum.com/user/13355/</uri>
			</author>
			<updated>2016-02-14T01:57:05Z</updated>
			<id>https://www.soliforum.com/post/116457/#p116457</id>
		</entry>