<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — design coming up from paper]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/13285/" />
	<updated>2016-01-05T14:38:14Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/13285/design-coming-up-from-paper/</id>
		<entry>
			<title type="html"><![CDATA[Re: design coming up from paper]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113315/#p113315" />
			<content type="html"><![CDATA[<p>the paper they give you is junk use gluesticks</p>]]></content>
			<author>
				<name><![CDATA[johnboyjr]]></name>
				<uri>https://www.soliforum.com/user/12832/</uri>
			</author>
			<updated>2016-01-05T14:38:14Z</updated>
			<id>https://www.soliforum.com/post/113315/#p113315</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: design coming up from paper]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113273/#p113273" />
			<content type="html"><![CDATA[<p>The magic number is half or less of your desired layer height. If you plan to print at .3 then you would need .15. if you plan to print at .1 then you would need .05. There is no magic number for all scenarios. You need to make adjustments for every print.</p><p>When you change rolls of filament all your settings will change such as temp and speed and so on.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2016-01-05T01:49:52Z</updated>
			<id>https://www.soliforum.com/post/113273/#p113273</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: design coming up from paper]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113271/#p113271" />
			<content type="html"><![CDATA[<p>I am new to this whole thing, but I believe you should lower the Z-offset so the extruder is a bit closer to the printing bed. Take it slow. The manual suggests the distance be the thickness of 4 sheets of paper. If your extruder is farther than that from the bed, drop it down a bit.</p>]]></content>
			<author>
				<name><![CDATA[chemist6.02e23]]></name>
				<uri>https://www.soliforum.com/user/13056/</uri>
			</author>
			<updated>2016-01-05T01:33:01Z</updated>
			<id>https://www.soliforum.com/post/113271/#p113271</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[design coming up from paper]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113232/#p113232" />
			<content type="html"><![CDATA[<p>I used the release paper that came with the printer. The design starts printing fine, but, part way through the design peels up from the release paoer?<br />John</p>]]></content>
			<author>
				<name><![CDATA[jgapril]]></name>
				<uri>https://www.soliforum.com/user/13142/</uri>
			</author>
			<updated>2016-01-04T14:33:44Z</updated>
			<id>https://www.soliforum.com/post/113232/#p113232</id>
		</entry>
</feed>