<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — nothing happening]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/13275/" />
	<updated>2016-01-04T00:44:20Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/13275/nothing-happening/</id>
		<entry>
			<title type="html"><![CDATA[Re: nothing happening]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113188/#p113188" />
			<content type="html"><![CDATA[<p>thank you so much, that did it---works great now</p>]]></content>
			<author>
				<name><![CDATA[jgapril]]></name>
				<uri>https://www.soliforum.com/user/13142/</uri>
			</author>
			<updated>2016-01-04T00:44:20Z</updated>
			<id>https://www.soliforum.com/post/113188/#p113188</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: nothing happening]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113179/#p113179" />
			<content type="html"><![CDATA[<p>Same thing happened to me. Mark is right. Follow the instructions to see to about &quot;4 sheets of paper&quot; height.</p>]]></content>
			<author>
				<name><![CDATA[chemist6.02e23]]></name>
				<uri>https://www.soliforum.com/user/13056/</uri>
			</author>
			<updated>2016-01-03T21:56:37Z</updated>
			<id>https://www.soliforum.com/post/113179/#p113179</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: nothing happening]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113164/#p113164" />
			<content type="html"><![CDATA[<p>Your z height is not set right.&nbsp; The z axis is starting to low. You will need to adjust it so its about .2 mm above.</p>]]></content>
			<author>
				<name><![CDATA[mark.burton]]></name>
				<uri>https://www.soliforum.com/user/10955/</uri>
			</author>
			<updated>2016-01-03T17:21:06Z</updated>
			<id>https://www.soliforum.com/post/113164/#p113164</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[nothing happening]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113155/#p113155" />
			<content type="html"><![CDATA[<p><span class="postimg"><img src="http://soliforum.com/i/?VouaRIh.jpg" alt="http://soliforum.com/i/?VouaRIh.jpg" /></span>OK, brand new-be here.<br />Just opened and attempted to print a sample, but it seems to be working however the nozzle just moves and scrapes the plate, no plastic.<br />John</p>]]></content>
			<author>
				<name><![CDATA[jgapril]]></name>
				<uri>https://www.soliforum.com/user/13142/</uri>
			</author>
			<updated>2016-01-03T16:19:53Z</updated>
			<id>https://www.soliforum.com/post/113155/#p113155</id>
		</entry>
</feed>