<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — XYZ default settings for slic3r]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/13266/" />
	<updated>2016-01-03T15:26:46Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/13266/xyz-default-settings-for-slic3r/</id>
		<entry>
			<title type="html"><![CDATA[Re: XYZ default settings for slic3r]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113149/#p113149" />
			<content type="html"><![CDATA[<p>I seem to remember the slow setting being 30mm/s but I could be wrong (no longer using xyz).<br />That&#039;s actually the speed I use when I want to print fast.</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2016-01-03T15:26:46Z</updated>
			<id>https://www.soliforum.com/post/113149/#p113149</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ default settings for slic3r]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113142/#p113142" />
			<content type="html"><![CDATA[<p>I thought the stock XYZ software used fixed settings?</p>]]></content>
			<author>
				<name><![CDATA[crazyewok]]></name>
				<uri>https://www.soliforum.com/user/12436/</uri>
			</author>
			<updated>2016-01-03T12:10:41Z</updated>
			<id>https://www.soliforum.com/post/113142/#p113142</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ default settings for slic3r]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113125/#p113125" />
			<content type="html"><![CDATA[<p>There is no such thing as default settings. Every printer is different and every roll of filament is different. The settings will change every time you load a new roll. Even the same color by the same vendor will be different from the last. </p><p>That is part of the printing process is to find the optimal settings for your machine and filament. Somebody might could give you some numbers but they will only get you in the ball park. I sold my Da Vinci so I don&#039;t have numbers to give you.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2016-01-03T04:05:54Z</updated>
			<id>https://www.soliforum.com/post/113125/#p113125</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[XYZ default settings for slic3r]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/113123/#p113123" />
			<content type="html"><![CDATA[<p>Just wondering what the default settings for a XYZ 1.0 AIO&nbsp; printing at 0.1mm on slow speed is if I was to to put into slic3cr?&nbsp; </p><p>Mainly speed and retraction settings?</p><p>Cant seem to find out anywere.</p><p>Want to put the default settings in then adjust from there.</p>]]></content>
			<author>
				<name><![CDATA[crazyewok]]></name>
				<uri>https://www.soliforum.com/user/12436/</uri>
			</author>
			<updated>2016-01-03T01:21:32Z</updated>
			<id>https://www.soliforum.com/post/113123/#p113123</id>
		</entry>
</feed>