<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — Printer drags through existing layers.]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/12658/" />
	<updated>2015-11-06T18:08:37Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/12658/printer-drags-through-existing-layers/</id>
		<entry>
			<title type="html"><![CDATA[Re: Printer drags through existing layers.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/109058/#p109058" />
			<content type="html"><![CDATA[<p>Check your calibration, I have had the same issue.</p><p>Happy Printing!</p>]]></content>
			<author>
				<name><![CDATA[Jimmyloopa]]></name>
				<uri>https://www.soliforum.com/user/12423/</uri>
			</author>
			<updated>2015-11-06T18:08:37Z</updated>
			<id>https://www.soliforum.com/post/109058/#p109058</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Printer drags through existing layers.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108393/#p108393" />
			<content type="html"><![CDATA[<p>Also check your bearing mounts</p>]]></content>
			<author>
				<name><![CDATA[mark.burton]]></name>
				<uri>https://www.soliforum.com/user/10955/</uri>
			</author>
			<updated>2015-10-27T22:15:47Z</updated>
			<id>https://www.soliforum.com/post/108393/#p108393</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Printer drags through existing layers.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108363/#p108363" />
			<content type="html"><![CDATA[<p>Have you checked if your bed is warped?&nbsp; If it is, grab one of <a href="http://www.ebay.com/itm/XYZPrinting-DaVinci-3D-Printer-Borosilicate-glass-and-heater-/252123636630?">these</a> and swap it in.&nbsp; I had similar issues, and kicked myself that I didn&#039;t replace the warped bed sooner, as having a non-warped bed dramatically upped my print quality.&nbsp; Swapping only takes about 10 minutes.</p>]]></content>
			<author>
				<name><![CDATA[SvdSinner]]></name>
				<uri>https://www.soliforum.com/user/10618/</uri>
			</author>
			<updated>2015-10-27T16:23:29Z</updated>
			<id>https://www.soliforum.com/post/108363/#p108363</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Printer drags through existing layers.]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108359/#p108359" />
			<content type="html"><![CDATA[<p>Hey there.<br />My 3d printer is draging through a existing layer when it prints. I can hear a creeeeeek sound and my desk starts to vibrate the nozzle only .05 too far down or something like that.</p>]]></content>
			<author>
				<name><![CDATA[DopeSkrit]]></name>