<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — XYZ 1.0A  Belt Break]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/12638/" />
	<updated>2015-10-29T13:12:55Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/12638/xyz-10a-belt-break/</id>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108502/#p108502" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>carl_m1968 wrote:</cite><blockquote><div class="quotebox"><cite>barry1685 wrote:</cite><blockquote><p>I believe its a 20 tooth gear with 3mm to 6mm width (you need to measure the other y belt width) doesn&#039;t matter what length it is, you can cut the new belt</p></blockquote></div><br /><p>If you cut it, how do you rejoin it into the small 3 inch loop needed to link the motor gear to the rear y drive gear?</p><p>As for measuring just a piece of string in place of the belt. Loop around and mark where joins then remove, tape at joint and measure.</p></blockquote></div><p>Yikes, didn&#039;t know it was THAT belt. you can&#039;t rejoin that belt.</p>]]></content>
			<author>
				<name><![CDATA[barry1685]]></name>
				<uri>https://www.soliforum.com/user/8171/</uri>
			</author>
			<updated>2015-10-29T13:12:55Z</updated>
			<id>https://www.soliforum.com/post/108502/#p108502</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108487/#p108487" />
			<content type="html"><![CDATA[<p>No,on crash. All components factory installed. I will lean toward belt quality.</p>]]></content>
			<author>
				<name><![CDATA[Beaverboat]]></name>
				<uri>https://www.soliforum.com/user/12404/</uri>
			</author>
			<updated>2015-10-29T02:15:04Z</updated>
			<id>https://www.soliforum.com/post/108487/#p108487</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108478/#p108478" />
			<content type="html"><![CDATA[<p>Could be too tight, pulleys misaligned, or could have just been a cheap belt.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-10-29T01:04:14Z</updated>
			<id>https://www.soliforum.com/post/108478/#p108478</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108477/#p108477" />
			<content type="html"><![CDATA[<p>no idea. Are you crashing the carriage?</p>]]></content>
			<author>
				<name><![CDATA[mark.burton]]></name>
				<uri>https://www.soliforum.com/user/10955/</uri>
			</author>
			<updated>2015-10-29T01:03:14Z</updated>
			<id>https://www.soliforum.com/post/108477/#p108477</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108460/#p108460" />
			<content type="html"><![CDATA[<p>Thanks Mark for the help. Any ideas of what would cause premature failure of belt?</p>]]></content>
			<author>
				<name><![CDATA[Beaverboat]]></name>
				<uri>https://www.soliforum.com/user/12404/</uri>
			</author>
			<updated>2015-10-28T21:53:27Z</updated>
			<id>https://www.soliforum.com/post/108460/#p108460</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108416/#p108416" />
			<content type="html"><![CDATA[<p>the number on the belt is 132-S2M<br />you can prolly get it here <br /><a href="http://www.kpaulindustrial.com/100-s2m-132.html">http://www.kpaulindustrial.com/100-s2m-132.html</a></p>]]></content>
			<author>
				<name><![CDATA[mark.burton]]></name>
				<uri>https://www.soliforum.com/user/10955/</uri>
			</author>
			<updated>2015-10-28T02:46:28Z</updated>
			<id>https://www.soliforum.com/post/108416/#p108416</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108397/#p108397" />
			<content type="html"><![CDATA[<p>If you would supply me with belt size that would be very much appreciated. My plan is to outsource replacement belt&nbsp; myself. XYZ customer support is rather slow. Thanks again.</p>]]></content>
			<author>
				<name><![CDATA[Beaverboat]]></name>
				<uri>https://www.soliforum.com/user/12404/</uri>
			</author>
			<updated>2015-10-27T22:53:16Z</updated>
			<id>https://www.soliforum.com/post/108397/#p108397</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108392/#p108392" />
			<content type="html"><![CDATA[<p>carriage belts you can fix to the carriage so it doesn&#039;t have to closed loop as the fixing it to the carriage closes the loop and you don&#039;t ever drag your carriage through the gears or idler. The y transfer belt you need to buy as the correct sized loop belt ,as it will loop through multiple times so any thing you used to close the loop will have to go through the gears and any idlers.</p><p> I can look at my small y drive belt and give you the number once mine is done printing.</p>]]></content>
			<author>
				<name><![CDATA[mark.burton]]></name>
				<uri>https://www.soliforum.com/user/10955/</uri>
			</author>
			<updated>2015-10-27T22:14:24Z</updated>
			<id>https://www.soliforum.com/post/108392/#p108392</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108366/#p108366" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>barry1685 wrote:</cite><blockquote><p>I believe its a 20 tooth gear with 3mm to 6mm width (you need to measure the other y belt width) doesn&#039;t matter what length it is, you can cut the new belt</p></blockquote></div><br /><p>If you cut it, how do you rejoin it into the small 3 inch loop needed to link the motor gear to the rear y drive gear?</p><p>As for measuring just a piece of string in place of the belt. Loop around and mark where joins then remove, tape at joint and measure.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-10-27T16:47:12Z</updated>
			<id>https://www.soliforum.com/post/108366/#p108366</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108365/#p108365" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>barry1685 wrote:</cite><blockquote><p>I believe its a 20 tooth gear with 3mm to 6mm width (you need to measure the other y belt width) doesn&#039;t matter what length it is, you can cut the new belt</p></blockquote></div><br /><p>If you cut it, how do you rejoin it into the small 3 inch loop needed to link the motor gear to the rear y drive gear?</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-10-27T16:44:30Z</updated>
			<id>https://www.soliforum.com/post/108365/#p108365</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108353/#p108353" />
			<content type="html"><![CDATA[<p>I believe its a 20 tooth gear with 3mm to 6mm width (you need to measure the other y belt width) doesn&#039;t matter what length it is, you can cut the new belt</p>]]></content>
			<author>
				<name><![CDATA[barry1685]]></name>
				<uri>https://www.soliforum.com/user/8171/</uri>
			</author>
			<updated>2015-10-27T13:37:54Z</updated>
			<id>https://www.soliforum.com/post/108353/#p108353</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108314/#p108314" />
			<content type="html"><![CDATA[<p>Not that I am attacking the OP, I am not. I am just curious how people break or even wear belts. I had a printer for a while that ran daily for 5 years and never broke or belt or even showed any wear on them. Could be be over tightening them or am I missing something here?</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-10-26T17:19:59Z</updated>
			<id>https://www.soliforum.com/post/108314/#p108314</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108310/#p108310" />
			<content type="html"><![CDATA[<p>It is the small belt &quot;Y&quot; axis. Unfortunately, I trashed the belt ,therefore I cannot verify belt size. If you have belt size available, could you please forward to me? XYZ stated it will be 2-3 days before they could get back to me on replacement. Thanks for the help.</p>]]></content>
			<author>
				<name><![CDATA[Beaverboat]]></name>
				<uri>https://www.soliforum.com/user/12404/</uri>
			</author>
			<updated>2015-10-26T16:47:53Z</updated>
			<id>https://www.soliforum.com/post/108310/#p108310</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108305/#p108305" />
			<content type="html"><![CDATA[<p>Which belt broke? gt2 belts work great for y axis&#039;s but x axis will need some sort of clip</p>]]></content>
			<author>
				<name><![CDATA[barry1685]]></name>
				<uri>https://www.soliforum.com/user/8171/</uri>
			</author>
			<updated>2015-10-26T14:45:32Z</updated>
			<id>https://www.soliforum.com/post/108305/#p108305</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: XYZ 1.0A  Belt Break]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/108291/#p108291" />
			<content type="html"><![CDATA[<p>well there are a few things you can do.<br />you can order a t2 timing belt just get the number off the broken belt. </p><p>if you do it right you can even make one for the x or y carriages&nbsp; by buying t2 timing belt and then fastening the loose ends to the carriages.</p>]]></content>
			<author>
				<name><![CDATA[mark.burton]]></name>
				<uri>https://www.soliforum.com/user/10955/</uri>
			</author>
			<updated>2015-10-26T02:22:45Z</updated>
			<id>https://www.soliforum.com/post/108291/#p108291</id>
		</entry>
</feed>