<?xml version="1.0" encoding="utf-8"?>
<feed xmlns="http://www.w3.org/2005/Atom">
	<title type="html"><![CDATA[SoliForum - 3D Printing Community — printing with white color]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/12519/" />
	<updated>2015-10-17T03:34:27Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/12519/printing-with-white-color/</id>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107835/#p107835" />
			<content type="html"><![CDATA[<p>Just want to back Revolve3D. I make spectacular filament with their pellets!<br />White, Black, Orange....all good stuff.</p>]]></content>
			<author>
				<name><![CDATA[AZERATE]]></name>
				<uri>https://www.soliforum.com/user/4188/</uri>
			</author>
			<updated>2015-10-17T03:34:27Z</updated>
			<id>https://www.soliforum.com/post/107835/#p107835</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107834/#p107834" />
			<content type="html"><![CDATA[<p>i do measure diameter for each new roll/color I get, and do a proper calibration for flow for each one, too - then save a profile for that particular roll/color. </p><p>getting temps set correctly for each one can sometimes be a challenge, tho - that info doesn&#039;t really get saved in the filament profiles&nbsp; <img src="https://www.soliforum.com/img/smilies/tongue.png" width="15" height="15" alt="tongue" /></p>]]></content>
			<author>
				<name><![CDATA[heartless]]></name>
				<uri>https://www.soliforum.com/user/10399/</uri>
			</author>
			<updated>2015-10-17T03:07:56Z</updated>
			<id>https://www.soliforum.com/post/107834/#p107834</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107789/#p107789" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>heartless wrote:</cite><blockquote><div class="quotebox"><cite>n2ri wrote:</cite><blockquote><p>yep and red/black even lower temps as those colors seem to ooze easier maybe even readjust flow rate a bit as if fililament is thicker than it is</p></blockquote></div><p>Red seems to be more of a pain for me than any other color - but black seems to want a slightly higher temps - on my printer anyway... <br />for me it seems lighter colors = lower temps, darker colors = higher temps... and glow in the dark&#039;s are way different - usually a fair bit lower than other colors of a similar material (ABS for me) If I run white &amp; yellow at 235C, the GITD is more like 220-225C</p><p>point is, temp should be checked/calibrated for each color.</p></blockquote></div><p>flow rate also and remeasure filament dia each roll for that too.</p>]]></content>
			<author>
				<name><![CDATA[n2ri]]></name>
				<uri>https://www.soliforum.com/user/795/</uri>
			</author>
			<updated>2015-10-16T17:05:15Z</updated>
			<id>https://www.soliforum.com/post/107789/#p107789</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107777/#p107777" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>n2ri wrote:</cite><blockquote><p>yep and red/black even lower temps as those colors seem to ooze easier maybe even readjust flow rate a bit as if fililament is thicker than it is</p></blockquote></div><p>Red seems to be more of a pain for me than any other color - but black seems to want a slightly higher temps - on my printer anyway... <br />for me it seems lighter colors = lower temps, darker colors = higher temps... and glow in the dark&#039;s are way different - usually a fair bit lower than other colors of a similar material (ABS for me) If I run white &amp; yellow at 235C, the GITD is more like 220-225C</p><p>point is, temp should be checked/calibrated for each color.</p>]]></content>
			<author>
				<name><![CDATA[heartless]]></name>
				<uri>https://www.soliforum.com/user/10399/</uri>
			</author>
			<updated>2015-10-16T15:25:38Z</updated>
			<id>https://www.soliforum.com/post/107777/#p107777</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107705/#p107705" />
			<content type="html"><![CDATA[<p>yep and red/black even lower temps as those colors seem to ooze easier maybe even readjust flow rate a bit as if fililament is thicker than it is</p>]]></content>
			<author>
				<name><![CDATA[n2ri]]></name>
				<uri>https://www.soliforum.com/user/795/</uri>
			</author>
			<updated>2015-10-15T22:09:01Z</updated>
			<id>https://www.soliforum.com/post/107705/#p107705</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107694/#p107694" />
			<content type="html"><![CDATA[<p>maybe I am lucky, but I have had no real problems using white filament - either PLA or ABS. <br />I have found that white generally likes a slightly lower temp than other colors (yellow too) by a few degrees, but with good calibrations it is no harder to work with than any other color.</p>]]></content>
			<author>
				<name><![CDATA[heartless]]></name>
				<uri>https://www.soliforum.com/user/10399/</uri>
			</author>
			<updated>2015-10-15T19:30:42Z</updated>
			<id>https://www.soliforum.com/post/107694/#p107694</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107651/#p107651" />
			<content type="html"><![CDATA[<p>that Revolve filament is great stuff. had pellets Filastruded (by another member here) for me that I won in Christmas giveaway with custom colors provided by Revolve to the guy that done it and we shared the filament. colors mix well with no fade/marbling.</p>]]></content>
			<author>
				<name><![CDATA[n2ri]]></name>
				<uri>https://www.soliforum.com/user/795/</uri>
			</author>
			<updated>2015-10-15T04:40:39Z</updated>
			<id>https://www.soliforum.com/post/107651/#p107651</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107584/#p107584" />
			<content type="html"><![CDATA[<p>I use the white PLA we sell. I would be happy to send out samples and provide photos of what I have printed with it.</p>]]></content>
			<author>
				<name><![CDATA[Revolve3D]]></name>
				<uri>https://www.soliforum.com/user/5822/</uri>
			</author>
			<updated>2015-10-14T16:40:01Z</updated>
			<id>https://www.soliforum.com/post/107584/#p107584</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107579/#p107579" />
			<content type="html"><![CDATA[<p>I use White Hatchbox PLA with great results.</p>]]></content>
			<author>
				<name><![CDATA[widespreaddeadhead]]></name>
				<uri>https://www.soliforum.com/user/9121/</uri>
			</author>
			<updated>2015-10-14T16:16:35Z</updated>
			<id>https://www.soliforum.com/post/107579/#p107579</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107335/#p107335" />
			<content type="html"><![CDATA[<p>Here&#039;s your cup...&nbsp; <img src="https://www.soliforum.com/img/smilies/lol.png" width="15" height="15" alt="lol" /></p><p>I just went this morning for bloodwork at Kaiser, and they gave me a cup too.</p>]]></content>
			<author>
				<name><![CDATA[pirvan]]></name>
				<uri>https://www.soliforum.com/user/1357/</uri>
			</author>
			<updated>2015-10-10T18:53:10Z</updated>
			<id>https://www.soliforum.com/post/107335/#p107335</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107286/#p107286" />
			<content type="html"><![CDATA[<p>Thx for this answer! I was sure you guys were going to ask me to go take a piss test!!!</p>]]></content>
			<author>
				<name><![CDATA[icebob]]></name>
				<uri>https://www.soliforum.com/user/11781/</uri>
			</author>
			<updated>2015-10-09T23:53:44Z</updated>
			<id>https://www.soliforum.com/post/107286/#p107286</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107284/#p107284" />
			<content type="html"><![CDATA[<p>The colorant added to filament affects them a lot. Yes white is the worst. For a wonderful time try natural.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-10-09T23:49:15Z</updated>
			<id>https://www.soliforum.com/post/107284/#p107284</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[printing with white color]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/107283/#p107283" />
			<content type="html"><![CDATA[<p>Is it just me or white is tricky to print? I tried ABS and PLA same brand, prints are fine in black, orange, red, gray ect... but white,,, they look like a cow arse... start fine but getting delam, uneven layer ect... should I just avoid white and print with natural? Thx in advance.</p>]]></content>
			<author>
				<name><![CDATA[icebob]]></name>
				<uri>https://www.soliforum.com/user/11781/</uri>
			</author>
			<updated>2015-10-09T23:26:38Z</updated>
			<id>https://www.soliforum.com/post/107283/#p107283</id>
		</entry>
</feed>