	<title type="html"><![CDATA[SoliForum - 3D Printing Community — firt layer problem]]></title>
	<link rel="self" href="https://www.soliforum.com/feed/atom/topic/11834/" />
	<updated>2015-07-22T21:09:15Z</updated>
	<generator>PunBB</generator>
	<id>https://www.soliforum.com/topic/11834/firt-layer-problem/</id>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101766/#p101766" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>efes wrote:</cite><blockquote><p>it is an amateur Machine .... I would change the rod and replace with the quality you think what?</p></blockquote></div><p>Those are not cheap rods. I tried cutting one at a machine shop and it took 45 minutes with an industrial band saw. They are hardened and chromed.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-07-22T21:09:15Z</updated>
			<id>https://www.soliforum.com/post/101766/#p101766</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101760/#p101760" />
			<content type="html"><![CDATA[<p>it is an amateur Machine .... I would change the rod and replace with the quality you think what?</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2015-07-22T19:38:28Z</updated>
			<id>https://www.soliforum.com/post/101760/#p101760</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101759/#p101759" />
			<content type="html"><![CDATA[<p>If you turn the rod then yes it is warped. But most are warped to some extent on Da Vinci. So you just have to compensate for the warpage.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-07-22T19:25:59Z</updated>
			<id>https://www.soliforum.com/post/101759/#p101759</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101756/#p101756" />
			<content type="html"><![CDATA[<p>ok tomorrow I go change is the bed of glass... why when I turn the shaft extruder head moves?I do not understand the glass bed of the problem?</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2015-07-22T18:59:31Z</updated>
			<id>https://www.soliforum.com/post/101756/#p101756</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101751/#p101751" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>efes wrote:</cite><blockquote><p>shaft Y bend !!!</p><p>2 weeks ago I sent an email to XYZ ....<br />they are sent two shaft Y guaranteed<br />I changed and I still have the same problem!</p><p>look video <a href="https://youtu.be/niw1ZFHhfv4">https://youtu.be/niw1ZFHhfv4</a></p><p>user davinci you have same problem ? </p><p>the number one problem Y shaft bend <img src="https://www.soliforum.com/img/smilies/sad.png" width="15" height="15" alt="sad" /></p><p>i have send mail XYZ ... I await the return</p></blockquote></div><br /><p>It is not your Y that is bent. It the bed that your print builds on. They are warped on almost all of the da vinci printers. You have to go to a glass shop and get a piece of glass that is 3mm thick cut to your existing glass dimensions. Then mount this piece on top of the old piece using the existing hold downs.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-07-22T18:15:13Z</updated>
			<id>https://www.soliforum.com/post/101751/#p101751</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101749/#p101749" />
			<content type="html"><![CDATA[<p>shaft Y bend !!!</p><p>2 weeks ago I sent an email to XYZ ....<br />they are sent two shaft Y guaranteed<br />I changed and I still have the same problem!</p><p>look video <a href="https://youtu.be/niw1ZFHhfv4">https://youtu.be/niw1ZFHhfv4</a></p><p>user davinci you have same problem ? </p><p>the number one problem Y shaft bend <img src="https://www.soliforum.com/img/smilies/sad.png" width="15" height="15" alt="sad" /></p><p>i have send mail XYZ ... I await the return</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2015-07-22T18:02:23Z</updated>
			<id>https://www.soliforum.com/post/101749/#p101749</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101734/#p101734" />
			<content type="html"><![CDATA[<p>Your retraction is already 2,00 mm which seems OK. </p><p>However, each filament can have its own need for a specific retraction at a specific temperature. Usually, oozing during a move when you are not supposed to be extruding means the filament is too hot or the retraction is too small or not fast enough. Retracting too much can pull liquid filament back above the melt zone and can cause a jam. </p><p>So, play with your filament temps and retraction settings until it starts working with this filament. Keep a good record of what works for each filament you have.</p>]]></content>
			<author>
				<name><![CDATA[ggunners]]></name>
				<uri>https://www.soliforum.com/user/4235/</uri>
			</author>
			<updated>2015-07-22T14:20:46Z</updated>
			<id>https://www.soliforum.com/post/101734/#p101734</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101684/#p101684" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>evanalmighty wrote:</cite><blockquote><p>Can you post a screen shot of your extruder/retraction setting screen?</p></blockquote></div><p>He did, its the top image in his series.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-07-21T22:25:25Z</updated>
			<id>https://www.soliforum.com/post/101684/#p101684</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101682/#p101682" />
			<content type="html"><![CDATA[<p>Can you post a screen shot of your extruder/retraction setting screen?</p>]]></content>
			<author>
				<name><![CDATA[evanalmighty]]></name>
				<uri>https://www.soliforum.com/user/8801/</uri>
			</author>
			<updated>2015-07-21T22:22:56Z</updated>
			<id>https://www.soliforum.com/post/101682/#p101682</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101678/#p101678" />
			<content type="html"><![CDATA[<p>yes...</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2015-07-21T21:06:28Z</updated>
			<id>https://www.soliforum.com/post/101678/#p101678</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101677/#p101677" />
			<content type="html"><![CDATA[<p>Looks more like a retraction issue to me.&nbsp; Are you using Simplify3D?</p>]]></content>
			<author>
				<name><![CDATA[evanalmighty]]></name>
				<uri>https://www.soliforum.com/user/8801/</uri>
			</author>
			<updated>2015-07-21T21:05:22Z</updated>
			<id>https://www.soliforum.com/post/101677/#p101677</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101675/#p101675" />
			<content type="html"><![CDATA[<p>ok..<br />I retract what I have to change?</p><p><span class="postimg"><img src="http://soliforum.com/i/?a3gZ0XP.jpg" alt="http://soliforum.com/i/?a3gZ0XP.jpg" /></span></p><p><span class="postimg"><img src="http://soliforum.com/i/?PKWMrIo.jpg" alt="http://soliforum.com/i/?PKWMrIo.jpg" /></span></p><p><span class="postimg"><img src="http://soliforum.com/i/?VbP9oW3.jpg" alt="http://soliforum.com/i/?VbP9oW3.jpg" /></span></p><p>thx help</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2015-07-21T20:41:19Z</updated>
			<id>https://www.soliforum.com/post/101675/#p101675</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101673/#p101673" />
			<content type="html"><![CDATA[<p>You may have a warped bed. My XYZ printer bed is warped and does not allow an even 1st layer.</p><p>In addition, the temperature of the heated bed is hottest in the middle and coolest at the edges. You will have difficulty with the edges lifting as you approach the corners.</p><p>Note that all your open circles are in the same location of the object, left side in the picture with the red boxes. That would seem to point to a change in direction problem. Perhaps belt tightness or some other mechanical issue.</p><p>The lines in the blue boxes are just over extrusion. You may want to adjust your retraction settings to retract more on those moves.</p>]]></content>
			<author>
				<name><![CDATA[ggunners]]></name>
				<uri>https://www.soliforum.com/user/4235/</uri>
			</author>
			<updated>2015-07-21T20:31:03Z</updated>
			<id>https://www.soliforum.com/post/101673/#p101673</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101669/#p101669" />
			<content type="html"><![CDATA[<p>yes I try to understand the paper and a sheet of A4 I made the adjustment ....<br />I must still adjust the bed? even crush the paper?</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2015-07-21T19:57:13Z</updated>
			<id>https://www.soliforum.com/post/101669/#p101669</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: firt layer problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101666/#p101666" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>efes wrote:</cite><blockquote><p>hello<br />the hole does not close well?<br />it flows filament track?<br />thank you for helping me</p><p><span class="postimg"><img src="http://nsa37.casimages.com/img/2015/07/21/150721093606870188.jpg" alt="http://nsa37.casimages.com/img/2015/07/21/150721093606870188.jpg" /></span></p><p><span class="postimg"><img src="http://nsa38.casimages.com/img/2015/07/21/15072109360330624.jpg" alt="http://nsa38.casimages.com/img/2015/07/21/15072109360330624.jpg" /></span></p><p><span class="postimg"><img src="http://nsa37.casimages.com/img/2015/07/21/150721094302741392.jpg" alt="http://nsa37.casimages.com/img/2015/07/21/150721094302741392.jpg" /></span></p></blockquote></div><br /><p>Your bed is too far from the extruder. Your first layer should be squished down paper thin. Are you using the manual method posted in the XYZ section to adjust your bed?</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-07-21T19:46:33Z</updated>