			<title type="html"><![CDATA[Re: print part problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101592/#p101592" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>efes wrote:</cite><blockquote><p>this <a href="http://www.aliexpress.com/item/Free-shipping-20pcs-lot-1g-silver-GD460-thermal-conductive-compound-grease-paste-silicone-for-cpu-heatsink/1270975713.html">http://www.aliexpress.com/item/Free-shi … 75713.html</a> good ?</p></blockquote></div><p>It is not that. If you want something to replace it with, just use high temperature rtv. </p><br /><p><a href="http://www.amazon.com/Permatex-81160-High-Temp-Silicone-Gasket/dp/B0002UEN1A">http://www.amazon.com/Permatex-81160-Hi … B0002UEN1A</a></p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-07-20T22:29:57Z</updated>
			<id>https://www.soliforum.com/post/101592/#p101592</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: print part problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101589/#p101589" />
			<content type="html"><![CDATA[<p>this <a href="http://www.aliexpress.com/item/Free-shipping-20pcs-lot-1g-silver-GD460-thermal-conductive-compound-grease-paste-silicone-for-cpu-heatsink/1270975713.html">http://www.aliexpress.com/item/Free-shi … 75713.html</a> good ?</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2015-07-20T21:33:53Z</updated>
			<id>https://www.soliforum.com/post/101589/#p101589</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: print part problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101588/#p101588" />
			<content type="html"><![CDATA[<p>It is high temperature epoxy, only way to remove it is carefully chip at it with something without damaging the thermistor or it&#039;s wires. It might also dissolve in acetone if you take the extruder apart and soak the heat block in acetone.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-07-20T21:26:29Z</updated>
			<id>https://www.soliforum.com/post/101588/#p101588</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: print part problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101587/#p101587" />
			<content type="html"><![CDATA[<p>I get it!<br />head extruder completely blocked !!!!<br />I do not know why?<br />I completely disassemble clean ....</p><p><span class="postimg"><img src="http://soliforum.com/i/?E6EBVti.jpg" alt="http://soliforum.com/i/?E6EBVti.jpg" /></span></p><p>What is this glue on the thermistor?</p><p>thx</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2015-07-20T21:11:31Z</updated>
			<id>https://www.soliforum.com/post/101587/#p101587</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: print part problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101548/#p101548" />
			<content type="html"><![CDATA[<p>hello </p><p>normal dimension 9.60 i have 5.90 ....<br />problem davinci or .... my setup ?</p><p><span class="postimg"><img src="http://nsa37.casimages.com/img/2015/07/20/150720111404101002.jpg" alt="http://nsa37.casimages.com/img/2015/07/20/150720111404101002.jpg" /></span></p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2015-07-20T09:11:54Z</updated>
			<id>https://www.soliforum.com/post/101548/#p101548</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[print part problem]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/101533/#p101533" />
			<content type="html"><![CDATA[<p>hello</p><p>print this : <a href="http://www.thingiverse.com/thing:511668">http://www.thingiverse.com/thing:511668</a><br />top of the hole is not close?<br />please help !</p><br /><p><span class="postimg"><img src="http://nsa37.casimages.com/img/2015/07/20/150720124207313915.jpg" alt="http://nsa37.casimages.com/img/2015/07/20/150720124207313915.jpg" /></span></p><br /><p>my setup simplify3d</p><p><span class="postimg"><img src="http://nsa38.casimages.com/img/2015/07/20/150720123736992323.jpg" alt="http://nsa38.casimages.com/img/2015/07/20/150720123736992323.jpg" /></span></p><p><span class="postimg"><img src="http://nsa38.casimages.com/img/2015/07/20/150720123737266726.jpg" alt="http://nsa38.casimages.com/img/2015/07/20/150720123737266726.jpg" /></span></p><p><span class="postimg"><img src="http://nsa37.casimages.com/img/2015/07/20/150720123737725094.jpg" alt="http://nsa37.casimages.com/img/2015/07/20/150720123737725094.jpg" /></span></p><p><span class="postimg"><img src="http://nsa37.casimages.com/img/2015/07/20/15072012373810521.jpg" alt="http://nsa37.casimages.com/img/2015/07/20/15072012373810521.jpg" /></span></p><p><span class="postimg"><img src="http://nsa37.casimages.com/img/2015/07/20/150720123738453340.jpg" alt="http://nsa37.casimages.com/img/2015/07/20/150720123738453340.jpg" /></span></p><p><span class="postimg"><img src="http://nsa38.casimages.com/img/2015/07/20/150720123738900333.jpg" alt="http://nsa38.casimages.com/img/2015/07/20/150720123738900333.jpg" /></span></p><br /><p>thx help</p>]]></content>
			<author>
				<name><![CDATA[efes]]></name>
				<uri>https://www.soliforum.com/user/11160/</uri>
			</author>
			<updated>2015-07-19T22:40:00Z</updated>
			<id>https://www.soliforum.com/post/101533/#p101533</id>
		</entry>
</feed>