			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/97503/#p97503" />
			<content type="html"><![CDATA[<p>I found that after switching slicers I had forgot to set the retraction rate in cura, I reduced it and eliminated what I would have described as a snapping/popping sound during extrusion, I too originally thought moisture but like you the filament was only open for a day or so, might be something to check.</p>]]></content>
			<author>
				<name><![CDATA[FrozenRC]]></name>
				<uri>https://www.soliforum.com/user/10626/</uri>
			</author>
			<updated>2015-05-30T13:04:02Z</updated>
			<id>https://www.soliforum.com/post/97503/#p97503</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96954/#p96954" />
			<content type="html"><![CDATA[<p>Try using cat litter (only crystallized) it works wonders for drying out filament. I&#039;ve had xyz filament come with bubbles in the filament. It could also be a bad batch</p>]]></content>
			<author>
				<name><![CDATA[barry1685]]></name>
				<uri>https://www.soliforum.com/user/8171/</uri>
			</author>
			<updated>2015-05-25T14:22:58Z</updated>
			<id>https://www.soliforum.com/post/96954/#p96954</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96732/#p96732" />
			<content type="html"><![CDATA[<p>I will post a pic but I think my first layer problems are from too much oozing.</p>]]></content>
			<author>
				<name><![CDATA[barry1685]]></name>
				<uri>https://www.soliforum.com/user/8171/</uri>
			</author>
			<updated>2015-05-22T19:15:51Z</updated>
			<id>https://www.soliforum.com/post/96732/#p96732</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96731/#p96731" />
			<content type="html"><![CDATA[<p>And if I use the lower pla temp I get extruder jams</p>]]></content>
			<author>
				<name><![CDATA[M_Lynch]]></name>
				<uri>https://www.soliforum.com/user/10883/</uri>
			</author>
			<updated>2015-05-22T19:09:15Z</updated>
			<id>https://www.soliforum.com/post/96731/#p96731</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96730/#p96730" />
			<content type="html"><![CDATA[<p>I&#039;m using the normal ABS print temperature that the da Vinci uses which is about 215 to 220°C</p>]]></content>
			<author>
				<name><![CDATA[M_Lynch]]></name>
				<uri>https://www.soliforum.com/user/10883/</uri>
			</author>
			<updated>2015-05-22T19:06:42Z</updated>
			<id>https://www.soliforum.com/post/96730/#p96730</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96727/#p96727" />
			<content type="html"><![CDATA[<p>Hmm, that&#039;s not what I thought you meant. Not the same issue I had.<br />I&#039;m wondering if it might be temperature related. Black can be tricky to print at the best of times, this stuff maybe needs a lower extruder temp.<br />What extruder temp are you using ?</p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2015-05-22T18:47:11Z</updated>
			<id>https://www.soliforum.com/post/96727/#p96727</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96725/#p96725" />
			<content type="html"><![CDATA[<p>My first layer doesn&#039;t look like that. Its really messy though.</p>]]></content>
			<author>
				<name><![CDATA[barry1685]]></name>
				<uri>https://www.soliforum.com/user/8171/</uri>
			</author>
			<updated>2015-05-22T18:42:44Z</updated>
			<id>https://www.soliforum.com/post/96725/#p96725</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96724/#p96724" />
			<content type="html"><![CDATA[<p><span class="postimg"><img src="http://soliforum.com/i/?D9Veb4d.jpg" alt="http://soliforum.com/i/?D9Veb4d.jpg" /></span></p>]]></content>
			<author>
				<name><![CDATA[M_Lynch]]></name>
				<uri>https://www.soliforum.com/user/10883/</uri>
			</author>
			<updated>2015-05-22T18:27:50Z</updated>
			<id>https://www.soliforum.com/post/96724/#p96724</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96721/#p96721" />
			<content type="html"><![CDATA[<p>I made a dry box a while back, and I keep all of my filament in it, so it will stay dry. I will upload a picture of what it happening if I can ever get one to load.</p>]]></content>
			<author>
				<name><![CDATA[M_Lynch]]></name>
				<uri>https://www.soliforum.com/user/10883/</uri>
			</author>
			<updated>2015-05-22T18:11:32Z</updated>
			<id>https://www.soliforum.com/post/96721/#p96721</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96692/#p96692" />
			<content type="html"><![CDATA[<p>I would agree with Carl. I had the moisture problem myself with a roll of 3rd party ABS.<br />My prints were a mess, looked like someone had taken a cheese grater to them.<br />I put the ABS in an airing cupboard overnight and it printed fine after that.<br />I now store all my filament in these .... <a href="http://www.thingiverse.com/thing:457359">http://www.thingiverse.com/thing:457359</a></p>]]></content>
			<author>
				<name><![CDATA[scobo]]></name>
				<uri>https://www.soliforum.com/user/6872/</uri>
			</author>
			<updated>2015-05-22T15:43:38Z</updated>
			<id>https://www.soliforum.com/post/96692/#p96692</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96683/#p96683" />
			<content type="html"><![CDATA[<p>My first layer is always chunky. This happens to me when the speed is set lower. I think my extrusion rate may be too much. Either that or I have a moisture problem as well. Sometimes you see these small tiny chunks that come out of the extruder. Temp change doesn&#039;t really help this.</p>]]></content>
			<author>
				<name><![CDATA[barry1685]]></name>
				<uri>https://www.soliforum.com/user/8171/</uri>
			</author>
			<updated>2015-05-22T13:42:45Z</updated>
			<id>https://www.soliforum.com/post/96683/#p96683</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96665/#p96665" />
			<content type="html"><![CDATA[<div class="quotebox"><cite>M_Lynch wrote:</cite><blockquote><p>I just open the filament today, and it is stored in a dry box. Whenever I print the first layer cracks start forming in the center of the print, and those areas start to lift off the print bed.</p></blockquote></div><p>Do you mean the layers are seperating?</p><p>A picture would help as well as setttingd like temp on extruder and bed. Thr speeds your printing at and so fourth.&nbsp; Its alwsys good to give as much info as possible when looking for help with problems and ad the old saying goes a picture is worth a thousand words.</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-05-22T08:55:52Z</updated>
			<id>https://www.soliforum.com/post/96665/#p96665</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96664/#p96664" />
			<content type="html"><![CDATA[<p>I just open the filament today, and it is stored in a dry box. Whenever I print the first layer cracks start forming in the center of the print, and those areas start to lift off the print bed.</p>]]></content>
			<author>
				<name><![CDATA[M_Lynch]]></name>
				<uri>https://www.soliforum.com/user/10883/</uri>
			</author>
			<updated>2015-05-22T08:41:12Z</updated>
			<id>https://www.soliforum.com/post/96664/#p96664</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96663/#p96663" />
			<content type="html"><![CDATA[<p>Your filament has set around in the open and absorbed too much moisture.&nbsp; That moisture is turning to steam as it heats and causing the bubbles. You could try storing the filament in an air tight container with rice or other dissicant. </p><p>In the future never open filament till you want to use it, and store open filament in an air tight container with something to absorb moisture just in case.</p><p>You could also be printing too hot but you would know by the smell</p>]]></content>
			<author>
				<name><![CDATA[carl_m1968]]></name>
				<uri>https://www.soliforum.com/user/7731/</uri>
			</author>
			<updated>2015-05-22T08:33:24Z</updated>
			<id>https://www.soliforum.com/post/96663/#p96663</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Prints bubbling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/96662/#p96662" />
			<content type="html"><![CDATA[<p>I finally got my da Vinci 1.0 to work again. I did a few test prints and it seemed to work just fine, but whenever I print larger objects the print seems to bubble, any ideas? <br />Thanks,<br />Mark Lynch</p>]]></content>
			<author>
				<name><![CDATA[M_Lynch]]></name>
				<uri>https://www.soliforum.com/user/10883/</uri>
			</author>
			<updated>2015-05-22T08:19:21Z</updated>
			<id>https://www.soliforum.com/post/96662/#p96662</id>