		<entry>
			<title type="html"><![CDATA[Re: Received Some dirty filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/92627/#p92627" />
			<content type="html"><![CDATA[<p>Yes have them send you a new one.</p>]]></content>
			<author>
				<name><![CDATA[metaldrgn]]></name>
				<uri>https://www.soliforum.com/user/2429/</uri>
			</author>
			<updated>2015-04-10T14:41:50Z</updated>
			<id>https://www.soliforum.com/post/92627/#p92627</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Received Some dirty filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/88648/#p88648" />
			<content type="html"><![CDATA[<p>I&#039;ve had that happen I just wrapped a micro fiber cloth around the filament before it entered the printer enclosure.&nbsp; Wrapped that with some tape to hold it in place.&nbsp; I printed that whole roll without issue.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2015-03-07T01:09:21Z</updated>
			<id>https://www.soliforum.com/post/88648/#p88648</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Received Some dirty filament]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/88645/#p88645" />
			<content type="html"><![CDATA[<p>I just received some filament that had the plastic bag break during shipping, and as a result, the filament is very dusty and dirty. Is there a good way to clean the filament up?</p>]]></content>
			<author>
				<name><![CDATA[Ggalisky]]></name>
				<uri>https://www.soliforum.com/user/5970/</uri>
			</author>
			<updated>2015-03-07T00:45:55Z</updated>
			<id>https://www.soliforum.com/post/88645/#p88645</id>
		</entry>