			<title type="html"><![CDATA[Re: Does anyone have an extra bulldog xl 1.75mm bowden coupling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/86332/#p86332" />
			<content type="html"><![CDATA[<p>Here is my solution:<br /><span class="postimg"><img src="http://i.imgur.com/fxVUaw0.jpg" alt="http://i.imgur.com/fxVUaw0.jpg" /></span><br /><span class="postimg"><img src="http://i.imgur.com/Jpuyo89.jpg" alt="http://i.imgur.com/Jpuyo89.jpg" /></span><br /><span class="postimg"><img src="http://i.imgur.com/l7uQ55M.jpg" alt="http://i.imgur.com/l7uQ55M.jpg" /></span><br /><span class="postimg"><img src="http://i.imgur.com/iZuUySt.jpg" alt="http://i.imgur.com/iZuUySt.jpg" /></span><br /><span class="postimg"><img src="http://i.imgur.com/HXId4Dz.jpg" alt="http://i.imgur.com/HXId4Dz.jpg" /></span><br /><span class="postimg"><img src="http://i.imgur.com/WUZD3zL.jpg" alt="http://i.imgur.com/WUZD3zL.jpg" /></span></p><p>If you want the files I can post them. I had to use heat (PLA) to get these parts to mold correctly to the coupling. Re designing the pieces with an ID of 9.25mm would be a way to avoid using PLA.</p>]]></content>
			<author>
				<name><![CDATA[Ggalisky]]></name>
				<uri>https://www.soliforum.com/user/5970/</uri>
			</author>
			<updated>2015-02-20T05:46:36Z</updated>
			<id>https://www.soliforum.com/post/86332/#p86332</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Does anyone have an extra bulldog xl 1.75mm bowden coupling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/85785/#p85785" />
			<content type="html"><![CDATA[<p>As a temporary solution I designed and used this.&nbsp; It utilizes the clip from the E3d.<br /><span class="postimg"><img src="http://i.imgur.com/SmA3wEh.jpg" alt="http://i.imgur.com/SmA3wEh.jpg" /></span><br />It is no permanent solution that&#039;s for sure.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2015-02-17T17:55:45Z</updated>
			<id>https://www.soliforum.com/post/85785/#p85785</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Does anyone have an extra bulldog xl 1.75mm bowden coupling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/85783/#p85783" />
			<content type="html"><![CDATA[<p>Maybe you could design and print one that works?&nbsp; Just tweak your widths very carefully and set it to spiral vase mode.&nbsp; Nylon would probably work or maybe even ninjaflex.</p>]]></content>
			<author>
				<name><![CDATA[mdrVB6]]></name>
				<uri>https://www.soliforum.com/user/4377/</uri>
			</author>
			<updated>2015-02-17T17:48:03Z</updated>
			<id>https://www.soliforum.com/post/85783/#p85783</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Does anyone have an extra bulldog xl 1.75mm bowden coupling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/85758/#p85758" />
			<content type="html"><![CDATA[<p>That sounds like a good idea but the tubing that came with my bulldog is simply the wrong size.<br />I am no Bowden expert but I would think that having the ID close to the size filament we are using is important? </p><br /><p>From left to right <br />E3d ID about 2mm<br />Bulldog about 3mm<br />Bulldog about 4mm</p><p><span class="postimg"><img src="http://i.imgur.com/Sbf3udF.jpg" alt="http://i.imgur.com/Sbf3udF.jpg" /></span></p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2015-02-17T16:09:27Z</updated>
			<id>https://www.soliforum.com/post/85758/#p85758</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Does anyone have an extra bulldog xl 1.75mm bowden coupling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/85710/#p85710" />
			<content type="html"><![CDATA[<p>The bulldog uses a larger OD tube than E3D. I used an exacto to whittle down the end of the tube until it fit the E3D coupling.</p>]]></content>
			<author>
				<name><![CDATA[IanJohnson]]></name>
				<uri>https://www.soliforum.com/user/14/</uri>
			</author>
			<updated>2015-02-17T05:35:59Z</updated>
			<id>https://www.soliforum.com/post/85710/#p85710</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Does anyone have an extra bulldog xl 1.75mm bowden coupling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/85689/#p85689" />
			<content type="html"><![CDATA[<p>Let me know what you come up with.&nbsp; I&#039;m currently dealing with the same issue.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2015-02-17T01:56:53Z</updated>
			<id>https://www.soliforum.com/post/85689/#p85689</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Does anyone have an extra bulldog xl 1.75mm bowden coupling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/85678/#p85678" />
			<content type="html"><![CDATA[<p>Hmm maybe I need to design and print an adapter to get my e3d bowden coupling to work.</p>]]></content>
			<author>
				<name><![CDATA[Ggalisky]]></name>
				<uri>https://www.soliforum.com/user/5970/</uri>
			</author>
			<updated>2015-02-17T01:00:04Z</updated>
			<id>https://www.soliforum.com/post/85678/#p85678</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Re: Does anyone have an extra bulldog xl 1.75mm bowden coupling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/85657/#p85657" />
			<content type="html"><![CDATA[<p>That&#039;s a loaded question.&nbsp; I have extras but none of the ones that came with my BulldogXL work with the tubing or fittings that E3d uses.</p>]]></content>
			<author>
				<name><![CDATA[wardjr]]></name>
				<uri>https://www.soliforum.com/user/2291/</uri>
			</author>
			<updated>2015-02-16T23:52:41Z</updated>
			<id>https://www.soliforum.com/post/85657/#p85657</id>
		</entry>
		<entry>
			<title type="html"><![CDATA[Does anyone have an extra bulldog xl 1.75mm bowden coupling?]]></title>
			<link rel="alternate" href="https://www.soliforum.com/post/85654/#p85654" />
			<content type="html"><![CDATA[<p>If anyone has an extra, send me a PM and we can work something out.</p>]]></content>
			<author>
				<name><![CDATA[Ggalisky]]></name>
				<uri>https://www.soliforum.com/user/5970/</uri>
			</author>
			<updated>2015-02-16T23:37:42Z</updated>
			<id>https://www.soliforum.com/post/85654/#p85654</id>
		</entry>
</feed>