Topic: Diagonal Pattern Issue
Heya,
A couple of days ago I started noticing these patterns on my prints. Any ideas what may cause this?
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Help/Repair/Maintenance → Diagonal Pattern Issue
Heya,
A couple of days ago I started noticing these patterns on my prints. Any ideas what may cause this?
Moire. You can use a ceramic or other non-conductive screwdriver to adjust the VREF on the board (the one that says E). Only a tiny turn is needed, though.
Thanks.
First I tested it and it was ~190mV.
Then I printed the test cube at 150mV, 170mV, 200mV, 230mV and 270mV. The results were always the same.
Should I try even higher or lower? Or should I try smaller increments?
BTW, this is a SD2