1

Topic: Sources for Kapton Tape

I'm going to compile a list of sources for Kapton tape, for when you need to replace the tape that comes stock from the Solidoodle factory.

Feel free to add any others you find.

2

Re: Sources for Kapton Tape

Solidoodle now offers replacement Kapton squares in the store. Check it out at http://store.solidoodle.com/index.php?r … mp;path=63

Former Solidoodle employee, no longer associated with the company.

3

Re: Sources for Kapton Tape

Excellent! Added to first post.

4

Re: Sources for Kapton Tape

"A 0.2mm Kapton square for your Solidoodle 3D printer. This square is slightly thicker than the 1mm square that came installed in your printer. Comes pre cut into a conveniant square for easy instalation."

.2mm is not thicker than 1mm....

5

Re: Sources for Kapton Tape

Heh, looks like a type-o...

6

Re: Sources for Kapton Tape

@supporttech

I want to add 3 extra kapton squares to my order without having to pay $34 international shipping in order to checkout of the store.

How can I pay just the $30 for the sqaures and someone there make note that my specific order should have the 3 extra squares in it when its eventually shipped?

7

Re: Sources for Kapton Tape

macmub wrote:

@supporttech

I want to add 3 extra kapton squares to my order without having to pay $34 international shipping in order to checkout of the store.

How can I pay just the $30 for the sqaures and someone there make note that my specific order should have the 3 extra squares in it when its eventually shipped?

E-mail me and we will set something up. We are working on changing the store so that orders are easier to alter.

Former Solidoodle employee, no longer associated with the company.

8

Re: Sources for Kapton Tape

Its all been organised.
I payed $30 into Sam's paypal on the 21/8

My order is #2284

Maybe double check its all still ok. My printer should ship in the next few weeks.
I can imagine with how busy you guys are, there is a good chance I will get the printer sans extra squares.

Thanks

9

Re: Sources for Kapton Tape

I noticed earlier 3dprintergear in australia have a 33m roll of 140mm tape for $40
not quite the ideal 150mm (i assume) but pretty good nonetheless.


http://www.3dprintergear.com.au/140mm_w … kap140.htm

10

Re: Sources for Kapton Tape

Stoney wrote:

I noticed earlier 3dprintergear in australia have a 33m roll of 140mm tape for $40
not quite the ideal 150mm (i assume) but pretty good nonetheless.


http://www.3dprintergear.com.au/140mm_w … kap140.htm

i bought a roll of 80mm wide off ebay for $22 from hong kong
i had a practice at applying to my pieces of glass im going to use as my printer bed. Its quite easy when its in front of you and not inside a small machine.

Only problem I have is i think its thin tape. Im pretty sure the tape solidoodle supply is thicker than standard kapton.
I can see the tape ive got would tear quite easily.

11

Re: Sources for Kapton Tape

macmub wrote:
Stoney wrote:

I noticed earlier 3dprintergear in australia have a 33m roll of 140mm tape for $40
not quite the ideal 150mm (i assume) but pretty good nonetheless.


http://www.3dprintergear.com.au/140mm_w … kap140.htm

i bought a roll of 80mm wide off ebay for $22 from hong kong
i had a practice at applying to my pieces of glass im going to use as my printer bed. Its quite easy when its in front of you and not inside a small machine.

Only problem I have is i think its thin tape. Im pretty sure the tape solidoodle supply is thicker than standard kapton.
I can see the tape ive got would tear quite easily.

Any chance we could get some pictures of your prints on glass? This would be great material for the official wiki.

Former Solidoodle employee, no longer associated with the company.

12

Re: Sources for Kapton Tape

I did a blog post about it - http://solidoodletips.wordpress.com/201 … t-surface/

13

Re: Sources for Kapton Tape

IanJohnson wrote:

I did a blog post about it - http://solidoodletips.wordpress.com/201 … t-surface/

Beautiful stuff!

Former Solidoodle employee, no longer associated with the company.

14 (edited by HelmutK 2012-10-19 18:40:15)

Re: Sources for Kapton Tape

I just bought a roll of 150mm x 100ft of 60micron Kapton tape from ebay for $25.19 shipped.

15

Re: Sources for Kapton Tape

Hi,

please add this source for Kapton Tape:

mueller-ahlhorn.com/en/products-materials/material/adhesive-tapes/polyimide-tapes/


The good thing is, that you can get various thicknesses and also cut to size shapes and tapes

16 (edited by Kvirre 2012-10-29 08:32:10)

Re: Sources for Kapton Tape

Hi,

I got a replacement-square delivered with my printer.
However, it does not seem to be any adhesive on it?

Can I expect the "glue" to remain on the platform when removing the old sheet?
How do I get about of replacing this?

17

Re: Sources for Kapton Tape

Kvirre wrote:

Hi,

I got a replacement-square delivered with my printer.
However, it does not seem to be any adhesive on it?

Can I expect the "glue" to remain on the platform when removing the old sheet?
How do I get about of replacing this?

It works like a sticker. You sure you've pulled the back off?

Former Solidoodle employee, no longer associated with the company.

18

Re: Sources for Kapton Tape

Grainger sells the Kapton Tape and Film. www.grainger.com

19

Re: Sources for Kapton Tape

I got a bunch for cheap at aliexpress.com back when I was doing BGA rework.

20

Re: Sources for Kapton Tape

Another source for kapton tape.  We are manufacturers of silicone PSA tape from China.  The commercial name of this kind of tape is kapton which is the trademark of Dupont company.

21

Re: Sources for Kapton Tape

Another source for polyimide tape

http://www.chrtape.com/film-polyimide-tape.aspx

their is also a lot of good technical data on kapton on  this sight.

Ultimaker S3.

22

Re: Sources for Kapton Tape

can i also mention amazon http://www.amazon.com/s/ref=nb_sb_sabc? … ton%20tape

23

Re: Sources for Kapton Tape

You guys are going to awaken polymide tape again, be careful...  haha

24 (edited by newq 2013-02-23 20:09:21)

Re: Sources for Kapton Tape

I added the initial list of kapton tape sources to the Soliwiki at http://www.soliwiki.com/Kapton_tape. I hope it's okay. Maybe someone else want's to expand on my stub.

25

Re: Sources for Kapton Tape

Here's 100 ft of 6" Kapton tape on ebay!  Looks like I can't post links yet but if you do a google search for 150mm kapton tape it's one of the first links.

Solidoodle 2 w/ heated bed