So the PS is the polystyrene plastic I listed in my above post? In the manual that came with the kits there is about 3 kanji then PS. If I can I will post a pic when I get home.
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Filastruder → Polymer Extrusion - A Brief Tutorial.
So the PS is the polystyrene plastic I listed in my above post? In the manual that came with the kits there is about 3 kanji then PS. If I can I will post a pic when I get home.
HIPS stands for high impact polystyrene, not polyethylene.
Sorry need to be more careful and read what I am looking at . was a long day yesterday but no excuse to post misinformation.
thanks for the correction
Tin .
I was going to scan the page that listed all the plastic's, but my scanner has carked it. When my library opens on Monday (ACMT) I will scan & upload the page then.
SoliForum - 3D Printing Community → Filastruder → Polymer Extrusion - A Brief Tutorial.
Powered by PunBB, supported by Informer Technologies, Inc.