1

Topic: Library of Photos.

So everyone knows what different things should likely look like. If the bed is too high or low at the start of printing, if it is not leveled from the corners, if the plastic coming through is intermittent, if it is too hot, cold, or whatever. When the free wheel arm is too tight versus too loose, etc. I think it would be good to see many, many photos taken by different people of virtually the same issues to confirm ones understanding of what their particular issue might end up being.

2

Re: Library of Photos.

You mean like this ?

http://reprap.org/wiki/Print_Troublesho … de#CAUSES:

3

Re: Library of Photos.

I think more amateur photos would be better. These photos are only one example and I am not sure they are as clear as they could be.

4

Re: Library of Photos.

This isn't as organized, but it's interesting - http://www.flickr.com/groups/3d-print-failures/

As print failures go, this one is pretty scary-

http://farm9.staticflickr.com/8388/8472258810_a336500719.jpg

5

Re: Library of Photos.

Thanks Ian. I feel better now!