Topic: Da Vainci Jr. Bed adhesion method?
Just tried printing on the tape that came with my Jr. and the print stuck a little too well. I had to remove the glass and use a chisel to get the print off.
Anyone else have better success?
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → XYZ Printing DaVinci → Da Vainci Jr. Bed adhesion method?
Just tried printing on the tape that came with my Jr. and the print stuck a little too well. I had to remove the glass and use a chisel to get the print off.
Anyone else have better success?
Just tried printing on the tape that came with my Jr. and the print stuck a little too well. I had to remove the glass and use a chisel to get the print off.
Anyone else have better success?
Use Elmers purple glue stick. It works much better on cold beds.
totalitarian wrote:Just tried printing on the tape that came with my Jr. and the print stuck a little too well. I had to remove the glass and use a chisel to get the print off.
Anyone else have better success?
Use Elmers purple glue stick. It works much better on cold beds.
Do you apply it straight to the glass?
carl_m1968 wrote:totalitarian wrote:Just tried printing on the tape that came with my Jr. and the print stuck a little too well. I had to remove the glass and use a chisel to get the print off.
Anyone else have better success?
Use Elmers purple glue stick. It works much better on cold beds.
Do you apply it straight to the glass?
yes and just wait fro the purple to go away. If you do have trouble removing the object just soak it and the glass in water.
totalitarian wrote:carl_m1968 wrote:Use Elmers purple glue stick. It works much better on cold beds.
Do you apply it straight to the glass?
yes and just wait fro the purple to go away. If you do have trouble removing the object just soak it and the glass in water.
Great I'll give it a go thanks
SoliForum - 3D Printing Community → XYZ Printing DaVinci → Da Vainci Jr. Bed adhesion method?