1 (edited by widespreaddeadhead 2015-12-07 16:41:18)

Topic: Hatchbox Wood filament

Great stuff! Printed using my standard PLA settings, only had to up the hotend temp by 10C. Printed a few duck calls and sanded and stained the one on the left. It also has a Bronzefill ring on it. The one on the right is lightly sanded on the top to show color difference.

Post's attachments

duck call.jpg 1.25 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
FolgerTech acrylic i3 - Titan - e3dv6 - OctoPi
FuseBox 1.4 CoreXY x2 - e3dv6cano/e3dv6 - Graphic Smart Display
Solidoodle Workbench - cable chain - traditional z-axis endstop - OctoPi
Lulzbot TAZ 5, Makerbot Mini

2

Re: Hatchbox Wood filament

That's pretty good!  Does it seem that the printed duck call has the same acoustic properties as a 'real' wooden one?

3

Re: Hatchbox Wood filament

I'm far from an expert, but it sure sounds like a duck! The reed is 3d printed and I think, like a few people in the thingiverse comments mentioned, if I cut some plastic from some electronics packaging, it'll be much louder.

FolgerTech acrylic i3 - Titan - e3dv6 - OctoPi
FuseBox 1.4 CoreXY x2 - e3dv6cano/e3dv6 - Graphic Smart Display
Solidoodle Workbench - cable chain - traditional z-axis endstop - OctoPi
Lulzbot TAZ 5, Makerbot Mini

4

Re: Hatchbox Wood filament

Printed this for Valentine's Day!

http://soliforum.com/i/?iGbtgsT.jpg

FolgerTech acrylic i3 - Titan - e3dv6 - OctoPi
FuseBox 1.4 CoreXY x2 - e3dv6cano/e3dv6 - Graphic Smart Display
Solidoodle Workbench - cable chain - traditional z-axis endstop - OctoPi
Lulzbot TAZ 5, Makerbot Mini

5

Re: Hatchbox Wood filament

That's one of the best prints I've ever seen. What was your process for finishing?

Printit 8.10 printer
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on
Filawinder and Filastruder #1870.....worth every penny!

6

Re: Hatchbox Wood filament

Sanded down until the layer lines disappeared, applied stain and let dry, then one coat of polyurethane. It's that easy. I used a plastic bristle brush to buff the rough outside down, planning on applying another coat of polyu, but I liked the finish... and so did she!

FolgerTech acrylic i3 - Titan - e3dv6 - OctoPi
FuseBox 1.4 CoreXY x2 - e3dv6cano/e3dv6 - Graphic Smart Display
Solidoodle Workbench - cable chain - traditional z-axis endstop - OctoPi
Lulzbot TAZ 5, Makerbot Mini

7

Re: Hatchbox Wood filament

Hey Widespreadedhead, That does look great! I printed an owl in the hatchbox pla, and tried to put some minwax stain on it but it didn't seem to take at all. I didn't stain just to see if that made a difference but any thoughts on this?

8

Re: Hatchbox Wood filament

HyruleJedi86 wrote:

Hey Widespreadedhead, That does look great! I printed an owl in the hatchbox pla, and tried to put some minwax stain on it but it didn't seem to take at all. I didn't stain just to see if that made a difference but any thoughts on this?

Did you sand it first? Essentially you want to treat this just like wood. So my plan of action would be:

Print
Sand
Clean dust, etc off...
stain(apply, wipe off excess, let sit for much longer then the can says, wipe again, let dry)
Apply clear coat, lightly sand, and repeat for desired finish.

FolgerTech acrylic i3 - Titan - e3dv6 - OctoPi
FuseBox 1.4 CoreXY x2 - e3dv6cano/e3dv6 - Graphic Smart Display
Solidoodle Workbench - cable chain - traditional z-axis endstop - OctoPi
Lulzbot TAZ 5, Makerbot Mini

9

Re: Hatchbox Wood filament

did you use support for the valentine print ??

Soliddoodle 4 stock w glass bed
Folger Tech Prusa 2020 upgraded to  ED3v6 and titan extruder
Marlin/Repetier Host/ Slic3r and Cura

10 (edited by JeremyLGSiegfried 2017-01-12 02:14:26)

Re: Hatchbox Wood filament

Awesome! This is why I'm trying to save up for hardened nozzles...and materials to throw in my Filastruder. Maybe I should buy a roll and see how homemade composite filament compares...

Filastruder 2607 w/ Filawinder @1.75mm.
Dual-extruder MaxMicron Prusa Mendel: RAMPS 1.4 w/ Repetier Firmware+Full Graphic LCD Controller, stock hotends, injection molded bowden extruders w/ hobbed gears, insulated enclosure w/ 2 heat lamps, RPi 2B+ w/ Repetier Server.
0.1-0.2mm layer height, heated bed w/ PEI surface, inductive-sensor autolevel, 0.5mm to 0.2mm nozzle diameters.

11

Re: Hatchbox Wood filament

I did use support, you might be able to get away without support on the mothers head at 0.1mm or better, but the arms will definitely need supports.

FolgerTech acrylic i3 - Titan - e3dv6 - OctoPi
FuseBox 1.4 CoreXY x2 - e3dv6cano/e3dv6 - Graphic Smart Display
Solidoodle Workbench - cable chain - traditional z-axis endstop - OctoPi
Lulzbot TAZ 5, Makerbot Mini