1

Topic: Who needs a good laugh today?

I've been experiencing some very slow extrusion the last couple of weeks. Once I reached the 2in/pm point, I reached out to elmoret to help me narrow it down. After a slight learning curve for home extrusion, I've had nothing but success with my Filastruder v1.6 and only speak the highest of his products.

So once I finally found some time to figure this out, I unmounted from the wall and set it down when I noticed what looked like a section of a washer. I never inspected the thrust bearing or lubricated it since assembly, so I now present to you the next hilarious installment of "Why You Should Listen To Tim".
http://i.imgur.com/UyJDbBX.jpg

http://i.imgur.com/XjUOZgZ.jpg

http://i.imgur.com/xg3SvDy.jpg

Inspect your thrust bearing and lubricate as needed. I hope everyone got as much of a laugh out of this as I did! big_smile

Printit Mason and Printit Horizon printers
Multiple SD2s- Bulldog XL, E3D v5/v6/Lite6, Volcano, Hobb Goblin, Titan, .9 motor, Lawsy carriages, direct Y drive, fishing line...the list goes on
Filawinder and Filastruder #1870.....worth every penny!

2

Re: Who needs a good laugh today?

Was it making any noise?

3

Re: Who needs a good laugh today?

lots of noise lmao

Sd4 #9080 with a glass bed. E3d chimera duel extruder. Paste extruder , duet wifi.
Lawsy carriages. linear bearings. Y axis direct drive, Kinect scanner
SD4#8188 glass bed, lawsly carriages, E3d v6, octoprint http://www.ustream.tv/channel/hotrod96z28
Filastruder/filawinder, Custom Delta 300mm x 600mm

4

Re: Who needs a good laugh today?

It did make a grinding sound at random, but I figured it was the stall protection board or some debris passing through. The latter is mostly unlikely with my routine, so I didn't pay much attention since I was getting great consisten. The older motors sub-v2.0 are louder to confirm what kronikabuse aptly stated.

This is entirely user error/neglect for anyone keeping score. My post is more of a public service message....and I'm still laughing in high spirits smile